David Carr wrote:
> 
> We are having a butterfingers problem in our lab and I am seeking some
> advice.  I am trying to find out if there is some product (e.g. plastic,
> resin) that we can use to coat the outside of some of our more delicate (and
> expensive) glassware to prevent or reduce the amount of breakage we have
> been experiencing.
> 
> Something commercially available would be preferable, but I'm open to almost
> anything.
> 
> Thanks for any assistance you can provide
> 
> Dr. David Carr
> Department of Physiology
> Northwestern University

Hello David,
If it must not be especially resistant to anything (heat, chemicals) You
can find a kind of rubber paint in do-it-yourself-stores, its normally
used to coat hammer shafts or handles of pliers (should at least be
resistant to oil, used on tools?) It produces a 1-2 mm thick film of
rubber like plastic. Don t know if it works on glass lab ware, but maybe
it s a hint to follow up^�
Moritz
Institute of cell biology
ETH Zurich
Switzerland


-- 
Paul J. Franklin (moderator - sci.chem.organic.synthesis) 
http://chemistry.gsu.edu/post_docs/koen/wnewshp.html
Georgia State University <chepjf@panther.gsu.edu>
Atlanta, GA
Thread Navigation

This is a paginated view of messages in the thread with full content displayed inline.

Messages are displayed in chronological order, with the original post highlighted in green.

Use pagination controls to navigate through all messages in large threads.

Back to All Threads