Hi there, I'm wondering if anyone out there has any suggestions for formulating a zero shrink claybody. I work with large amounts of solid clay which have interfitting parts. It is crucial that these parts do not warp (which they have been doing). I've tried adding up to 50% grog but I'm still not happy with its overall warpage/shrinkage. Any recipes or suggestions you might have would be greatly appreciated! Thanks in advanced, Carlo in Vancouver E-mail: ricc@direct.ca
Technical Details
Message-ID:
<4n41nl$3g7@aphex.direct.ca>Path:
arc1-ca.pugleaf.net!unknown!not-for-mailShow Full Headers
Complete Article Headers
X-Google-Language: ENGLISH,ASCII-7-bit X-Google-Thread: 107990,e466e424f77da1cf,start X-Google-Attributes: gid107990,public X-Google-Thread: 10ffb7,e466e424f77da1cf,start X-Google-Attributes: gid10ffb7,public From: ricc@direct.ca (riccardo sammarco) Subject: Zero shrink clay? Date: 1996/05/12 Message-ID: <4n41nl$3g7@aphex.direct.ca> X-Deja-AN: 154517586 content-type: Text/Plain; charset=US-ASCII organization: Canada Internet Direct Customer mime-version: 1.0 reply-to: ricc@direct.ca newsgroups: sci.materials.ceramics,bit.listserv.clayart