We make a product that is inserted into a pipe near a weld.  The
temperature can reach 1200 degrees celsius for short periods (5 or 10
minutes) when the flame from the welding rod touches the inserted tube.
The inserted tube has to be flexible so that it can be pulled around
bends in the pipe.  We have unsuccesfully tried silicon rubber (it burnt
- but only just) which suggest the temperature may not be so high.
Perhaps 800 degrees celsius.

Is there a material available that would suit the above application?

Thanks and regards.
-- 
Tony Marshall
Technical Details
Message-ID: <CXbniOAyPl4yEwBA@greyrock.demon.co.uk>
Path: arc1-ca.pugleaf.net!unknown!not-for-mail

Show Full Headers
Complete Article Headers
X-Google-Language: ENGLISH,ASCII-7-bit
X-Google-Thread: 107990,15d8ef9c2506bd3e,start
X-Google-Attributes: gid107990,public
X-Google-Thread: 1141dc,15d8ef9c2506bd3e,start
X-Google-Attributes: gid1141dc,public
X-Google-Thread: fe339,15d8ef9c2506bd3e,start
X-Google-Attributes: gidfe339,public
X-Google-Thread: 111a00,15d8ef9c2506bd3e,start
X-Google-Attributes: gid111a00,public
X-Google-Thread: f5cd5,15d8ef9c2506bd3e,start
X-Google-Attributes: gidf5cd5,public
X-Google-Thread: f7944,15d8ef9c2506bd3e,start
X-Google-Attributes: gidf7944,public
X-Google-Thread: 14d955,15d8ef9c2506bd3e,start
X-Google-Attributes: gid14d955,public
From: Tony Marshall <tony@greyrock.demon.co.uk>
Subject: Looking For Flexible Heat Resistant Material
Date: 1997/01/19
Message-ID: <CXbniOAyPl4yEwBA@greyrock.demon.co.uk>
X-Deja-AN: 210860831
distribution: world
x-nntp-posting-host: greyrock.demon.co.uk
organization: Greyrock
mime-version: 1.0
newsgroups: sci.materials.ceramics,fj.engr.materials,ntu.eng.material,sci.materials,sci.polymers,nctu.mat-sci-eng,fj.sci.chem