SEEKING SOURCE FOR THIN METAL FILMS

#178
From: ritley
Date: Thu, 27 Aug 1992 13:03
11 lines
812 bytes

Might anyone know of commercial sources for thin (and preferably single
crystal) FREESTANDING (i.e., unsupported by a substrate)
metal films, say 1000 A to a few microns?  

I have been told someone at the University of Denmark (?) routinely
produces high quality thin metal films, but I don't know the details
or whether anyone else produces these as well.

Many thanks!
Technical Details
Message-ID: <Btn89J.MG6@news.cso.uiuc.edu>
Path: arc1-ca.pugleaf.net!sparky!uunet!usc!sdd.hp.com!ux1.cso.uiuc.edu!news.cso.uiuc.edu!uimrl7.mrl.uiuc.edu!ritley

Show Full Headers
Complete Article Headers
Newsgroups: sci.materials
Path: arc1-ca.pugleaf.net!sparky!uunet!usc!sdd.hp.com!ux1.cso.uiuc.edu!news.cso.uiuc.edu!uimrl7.mrl.uiuc.edu!ritley
From: ritley@uimrl7.mrl.uiuc.edu ()
Subject: SEEKING SOURCE FOR THIN METAL FILMS
Message-ID: <Btn89J.MG6@news.cso.uiuc.edu>
Sender: usenet@news.cso.uiuc.edu (Net Noise owner)
Reply-To: ritley@uiucmrl.bitnet ()
Organization: Materials Research Lab
Date: Thu, 27 Aug 1992 13:03:19 GMT
Lines: 12