I'm hoping somebody can give me some help with these questions.

1.  What adhesives can bond high density polyethylene to rigid PVC or 
    HDPE to itself?  The bonds would be used in outdoor applications.

2.  What plastics would be resistant to soaking in hot transmission fluid?


Any help or guidance would be greatly appreciated.  Thanks a lot!

Take Care,
 
John 



----------------------------------------------------------------------------
                            
John Brennan 

a750288@pan.mc.ti.com 
Technical Details
Message-ID: <a750288.16@pan.mc.ti.com>
Path: arc1-ca.pugleaf.net!sparky!uunet!olivea!decwrl!sdd.hp.com!cs.utexas.edu!csc.ti.com!tilde.csc.ti.com!pan.mc.ti.com!a750288

Show Full Headers
Complete Article Headers
Path: arc1-ca.pugleaf.net!sparky!uunet!olivea!decwrl!sdd.hp.com!cs.utexas.edu!csc.ti.com!tilde.csc.ti.com!pan.mc.ti.com!a750288
From: a750288@pan.mc.ti.com (John E. Brennan)
Newsgroups: sci.materials
Subject: 2 plastics questions
Message-ID: <a750288.16@pan.mc.ti.com>
Date: 31 Aug 92 16:59:04 GMT
Sender: usenet@pan.mc.ti.com (USENET News System)
Organization: Texas Instruments Materials and Controls Group
Lines: 21