Re: 2 plastics questions

#184
From: William E. Johns;S23015
Date: Mon, 31 Aug 1992 20:49
27 lines
1671 bytes
In article <a750288.16@pan.mc.ti.com> a750288@pan.mc.ti.com (John E. Brennan) writes:
>I'm hoping somebody can give me some help with these questions.
>
>1.  What adhesives can bond high density polyethylene to rigid PVC or 
>    HDPE to itself?  The bonds would be used in outdoor applications.

I would guess that your best luck would be in bonding HDPE to PVC or itself
would be with HDPE itself.  Use it as a hot melt.

>2.  What plastics would be resistant to soaking in hot transmission fluid?

I just gotto believe there are lots and lots.  How hot?  Nylons, delrin,
PTFE, what's the application?
>
Ride Free,

Bill
________________________________________________________________
bill@wsuaix.csc.wsu.edu if you feel compelled to send email
johnsw@wsuvm1.csc.wsu.edu if you seriously expect an answer
AMA #500924   DoD #00314   WMTC #0002   SR= 2.125
FJ1200 R100GS/PD 740GLE  KotV KotRR KotD #0001  :-)
\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/

An adventure is only an inconvenience rightly understood.
An inconvenience is only an adventure wrongly considered.
                                               Chesterton
Technical Details
Message-ID: <1992Aug31.204952.29444@serval.net.wsu.edu>
Path: arc1-ca.pugleaf.net!sparky!uunet!cis.ohio-state.edu!zaphod.mps.ohio-state.edu!uakari.primate.wisc.edu!usenet.coe.montana.edu!news.u.washington.edu!serval!wsuaix.csc.wsu.edu!bill
References: <a750288.16@pan.mc.ti.com>

Show Full Headers
Complete Article Headers
Newsgroups: sci.materials
Path: arc1-ca.pugleaf.net!sparky!uunet!cis.ohio-state.edu!zaphod.mps.ohio-state.edu!uakari.primate.wisc.edu!usenet.coe.montana.edu!news.u.washington.edu!serval!wsuaix.csc.wsu.edu!bill
From: bill@wsuaix.csc.wsu.edu (William E. Johns;S23015)
Subject: Re: 2 plastics questions
Message-ID: <1992Aug31.204952.29444@serval.net.wsu.edu>
Sender: Bill Johns
Organization: Washington State University
References: <a750288.16@pan.mc.ti.com>
Date: Mon, 31 Aug 92 20:49:52 GMT
Lines: 27