Hi:

This message was originally posted to the optoelectronics forum. I am 
reposting it here, because it is not clear if Tony Springthorpe can get
direct access to the sci.materials newsgroup. All replies should go directly
to him at <ajs@bnr.ca>. Also he would appreciate it if someone could tell
him how he could post messages directly to this newsgroup in the future.

Thank you,

Sandip

Sandip Sengupta

>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>>
Subj:	Is there a source of AlN out there?

Return-Path: <ajs@bnr.ca>
From: "Anthony (A.J.) SpringThorpe" <0887329@bnr.ca>
Message-ID: <"3793 Fri Oct 16 08:53:40 1992"@bnr.ca>
To: opto.forum@gte.com
Subject: Is there a source of AlN out there?

This is a materials question, rather than a specific comment re'
optoelectronic devices. However,it does have relevance to being able to
prepare high quality epitaxial materials suitable for devices.
Specifically, I am trying to find a source of high purity aluminum
nitride so that I can get crucibles made for an MBE deposition system.
Bulk material is OK, but I would prefer a 100 um coating on a
conventional boron nitride crucible.
Anyone out there know where I might find such material, or another more
relevant NET where I might pose the same question?
Thanks for any help you can give.
Tony SpringThorpe @ BNR Ottawa
Technical Details
Message-ID: <1992Oct27.100338.1@woods.ulowell.edu>
Path: arc1-ca.pugleaf.net!sparky!uunet!noc.near.net!nic.umass.edu!umassd.edu!ulowell!woods.ulowell.edu!senguptas

Show Full Headers
Complete Article Headers
Newsgroups: sci.materials
Path: arc1-ca.pugleaf.net!sparky!uunet!noc.near.net!nic.umass.edu!umassd.edu!ulowell!woods.ulowell.edu!senguptas
From: senguptas@woods.ulowell.edu
Subject: AlN for MBE crucibles
Message-ID: <1992Oct27.100338.1@woods.ulowell.edu>
Lines: 36
Sender: usenet@ulowell.ulowell.edu (News manager - ulowell)
Organization: University of Lowell
Date: Tue, 27 Oct 1992 15:03:38 GMT