Re: Superconducting Gallium Arsenide... what's the latest?

#203
From: Stephan Petersen
Date: Mon, 17 Aug 1992 06:57
24 lines
1244 bytes
In article <8062@dirac.physics.purdue.edu>, parks@dirac.physics.purdue.edu
(Chris Parks) says:
>
>See:
>Phys. Rev. Lett., Vol. 66, pg. 3079 (1991)     <- original article
>Phys. Rev. Lett., Vol. 68, pg. 551,552 (1992)  <- comments and
>                                                  almost-retraction
>
>Chris Parks
>parks@physics.purdue.edu

Thanks for the references!

Stephan




+------------------------------------------------+
| Stephan Petersen                               |
|                                                |
| Bitnet/EARN: IFF291@DJUKFA11                   |
| Internet:    IFF291@zam001.zam.kfa-juelich.de  |
+------------------------------------------------+
Technical Details
Message-ID: <92230.085738IFF291@DJUKFA11.BITNET>
Path: arc1-ca.pugleaf.net!sparky!uunet!cis.ohio-state.edu!zaphod.mps.ohio-state.edu!darwin.sura.net!Sirius.dfn.de!zam103!djukfa11!iff291
References: <zyxm4pb@lynx.unm.edu> <13409@creare.COM> <92227.133615IFF291@DJUKFA11.BITNET> <8062@dirac.physics.purdue.edu>

Show Full Headers
Complete Article Headers
Path: arc1-ca.pugleaf.net!sparky!uunet!cis.ohio-state.edu!zaphod.mps.ohio-state.edu!darwin.sura.net!Sirius.dfn.de!zam103!djukfa11!iff291
From: IFF291@DJUKFA11.BITNET (Stephan Petersen)
Newsgroups: sci.materials
Subject: Re: Superconducting Gallium Arsenide... what's the latest?
Message-ID: <92230.085738IFF291@DJUKFA11.BITNET>
Date: 17 Aug 92 06:57:38 GMT
References: <zyxm4pb@lynx.unm.edu> <13409@creare.COM>
 <92227.133615IFF291@DJUKFA11.BITNET> <8062@dirac.physics.purdue.edu>
Organization: KFA  Forschungszentrum Juelich
Lines: 24