🚀 go-pugleaf

RetroBBS NetNews Server

Inspired by RockSolid Light RIP Retro Guy

Article View: sci.materials
Article #210

Adsorption of hydrocarbon vapour to metal surfaces

#210
From: Uwe Diekmann
Date: Thu, 20 Aug 1992 07:28
7 lines
858 bytes
I need information about the adsorption of hydrocarbons from gasoline vapour to metal (eg steel, aluminum)
surfaces. 
If you take a closed box made of blank metal filled with air and gasoline vapour, how much of
this vapour will adsorb to the metal surface, so that the concentration of hydrocarbons in the air decreases ?

Thanks, 
       Uwe Diekmann
Technical Details
Message-ID: <1992Aug20.072830.18327@newsserver.rrzn.uni-hannover.de>
Path: arc1-ca.pugleaf.net!sparky!uunet!wupost!darwin.sura.net!Sirius.dfn.de!solaris.rz.tu-clausthal.de!news!tw2!diekman

Show Full Headers
Complete Article Headers
Newsgroups: sci.materials
Path: arc1-ca.pugleaf.net!sparky!uunet!wupost!darwin.sura.net!Sirius.dfn.de!solaris.rz.tu-clausthal.de!news!tw2!diekman
From: diekman@tw2.iw.uni-hannover.de (Uwe Diekmann)
Subject: Adsorption of hydrocarbon vapour to metal surfaces
Message-ID: <1992Aug20.072830.18327@newsserver.rrzn.uni-hannover.de>
Sender: news@newsserver.rrzn.uni-hannover.de (News Service)
Reply-To: diekman@iw.uni-hannover.de
Organization: Sun Microsystems, Inc.
Date: Thu, 20 Aug 1992 07:28:30 GMT
Lines: 9