In article <x-jytdh@rpi.edu> vasisn@rpi.edu writes:
>
> I'm looking for a solvent or a combinations of two compatible solvent that would dissolve PET, nylon-6 and -66 without chemically degrading the material.
> would any one happen to have info in this regard?
>
>niraj vasishtha
>vasisn@rpi.edu
>
Yep, try furfuryl alcohol. Heat it gently, without flame. I have dissolved
any number of different nylons in the stuff--a great solvent for this type
of polymer.
Enjoy,
Bill
________________________________________________________________
bill@wsuaix.csc.wsu.edu if you feel compelled to send email
johnsw@wsuvm1.csc.wsu.edu if you seriously expect an answer
AMA #500924 DoD #00314 WMTC #0002 SR= 2.125
FJ1200 R100GS/PD 740GLE KotV KotRR KotD #0001 :-)
\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/
If you understand, things are just as they are;
If you do not understand, things are just as they are.
Zen verse
Technical Details
Message-ID:
<1992Aug21.161800.4727@serval.net.wsu.edu>Path:
arc1-ca.pugleaf.net!sparky!uunet!usc!rpi!usenet.coe.montana.edu!news.u.washington.edu!serval!wsuaix.csc.wsu.edu!billReferences:
<x-jytdh@rpi.edu>Show Full Headers
Complete Article Headers
Newsgroups: sci.materials Path: arc1-ca.pugleaf.net!sparky!uunet!usc!rpi!usenet.coe.montana.edu!news.u.washington.edu!serval!wsuaix.csc.wsu.edu!bill From: bill@wsuaix.csc.wsu.edu (William E. Johns;S23015) Subject: Re: dissolving nylon-6 and/or nylon-66 Message-ID: <1992Aug21.161800.4727@serval.net.wsu.edu> Sender: Bill Johns Organization: Washington State University References: <x-jytdh@rpi.edu> Date: Fri, 21 Aug 92 16:18:00 GMT Lines: 26