Re: Uses of Be

#232
From: medlin douglas l
Date: Tue, 13 Oct 1992 02:59
15 lines
1140 bytes
>>In article <1992Oct2.113921.2739@mtroyal.ab.ca>, dhayward@mtroyal.ab.ca writes:
>>>For years I have been interested in the present and future uses of
>>>Berrylium....

Beryllium is used frequently in applications where one wants to
avoid large amounts of secondary x-ray flourescence: thus it
is frequently used as an x-ray window material for x-ray detectors
and a material for making low background specimen stages for
analytical electron microscopes.  One advantage for x-ray
windows on SEMs is that Be is strong enough to withstand an atmosphere
of pressure even when the window is thin enough to
allow a large amount of x-ray transmission.  

Doug Medlin
dlmedli@snll-arpagw.llnl.gov
Technical Details
Message-ID: <332@snll-arpagw.llnl.gov>
Path: arc1-ca.pugleaf.net!sparky!uunet!know!hri.com!spool.mu.edu!agate!overload.lbl.gov!lll-winken!snll-arpagw!dlmedli
References: <1992Oct7.222241.148720@ns1.cc.lehigh.edu> <1992Oct10.130849.1024@dmp.csiro.au>

Show Full Headers
Complete Article Headers
Path: arc1-ca.pugleaf.net!sparky!uunet!know!hri.com!spool.mu.edu!agate!overload.lbl.gov!lll-winken!snll-arpagw!dlmedli
From: dlmedli@snll-arpagw.llnl.gov (medlin douglas l)
Newsgroups: sci.materials
Subject: Re: Uses of Be
Message-ID: <332@snll-arpagw.llnl.gov>
Date: 13 Oct 92 02:59:06 GMT
References: <1992Oct7.222241.148720@ns1.cc.lehigh.edu> <1992Oct10.130849.1024@dmp.csiro.au>
Organization: Sandia National Labs, Livermore, CA
Lines: 15