I am planning to begin my senior thesis, and one possible topic that
interests me is the disposal of bauxite tailings (red mud) and fly ash
through some combination of the two, perhaps making bricks or agglomerates
for concrete.  I know a little about them, but I was wondering if anyone
had specific knowledge about this, or could provide some good references on
red mud, fly ash, or combinations.  Thank you.

						Tony Prats

prats@bigvax.alfred.edu		Tony.Prats@lambada.oit.unc.edu


--
   The opinions expressed are not necessarily those of the University of
     North Carolina at Chapel Hill, the Campus Office for Information
        Technology, or the Experimental Bulletin Board Service.
           internet:  laUNChpad.unc.edu or 152.2.22.80
Technical Details
Message-ID: <1992Nov12.222835.5278@samba.oit.unc.edu>
Path: arc1-ca.pugleaf.net!sparky!uunet!stanford.edu!rock!concert!samba!usenet

Show Full Headers
Complete Article Headers
Newsgroups: sci.materials
Path: arc1-ca.pugleaf.net!sparky!uunet!stanford.edu!rock!concert!samba!usenet
From: Tony.Prats@launchpad.unc.edu (Tony Prats)
Subject: Red Mud and Fly ash
Message-ID: <1992Nov12.222835.5278@samba.oit.unc.edu>
Followup-To: prats@bigvax.alfred.edu
Summary: information wanted re: processing of red mud and fly ash
Keywords: Bauxite tailings, fly ash, re-use
Sender: usenet@samba.oit.unc.edu
Nntp-Posting-Host: lambada.oit.unc.edu
Organization: University of North Carolina Extended Bulletin Board Service
Date: Thu, 12 Nov 1992 22:28:35 GMT
Lines: 17