Article View: sci.materials
Article #268Re: Properties of titanium nitride
From: Mansig Kim
Date: Fri, 13 Nov 1992 15:55
Date: Fri, 13 Nov 1992 15:55
26 lines
1354 bytes
1354 bytes
In article <JAKE.92Nov11155601@nucst6.neep.wisc.edu> jake@nucst6.neep.wisc.edu (james blanchard) writes: > >Since there was some response to a recent request for the properties >of silicon nitride, I thought I'd post a similar request. Does anyone >have any information on the properties of titanium nitride? I'm >particularly interested in the strength of the material (yield >strength, rupture strength, etc.). Any numbers and or references >would be helpful. > > Thanks, >-- > > jake blanchard -- university of wisconsin - madison > blanchard@engr.wisc.edu OR jake@nucst6.neep.wisc.edu Since we have many requests about materials properties, do we have ftp site or free access site that provides properties information? I also need many materials properties. If I post news to get property information everytime I need, it will consume lots of news resources. Regards, Mansig
Technical Details
Message-ID:
<1e0j50INNf3c@bigboote.WPI.EDU>Path:
arc1-ca.pugleaf.net!sparky!uunet!know!hri.com!noc.near.net!bigboote.WPI.EDU!wpi.WPI.EDU!mkimReferences:
<JAKE.92Nov11155601@nucst6.neep.wisc.edu>Show Full Headers
Complete Article Headers
Path: arc1-ca.pugleaf.net!sparky!uunet!know!hri.com!noc.near.net!bigboote.WPI.EDU!wpi.WPI.EDU!mkim From: mkim@wpi.WPI.EDU (Mansig Kim) Newsgroups: sci.materials Subject: Re: Properties of titanium nitride Message-ID: <1e0j50INNf3c@bigboote.WPI.EDU> Date: 13 Nov 92 15:55:12 GMT References: <JAKE.92Nov11155601@nucst6.neep.wisc.edu> Distribution: sci Organization: Worcester Polytechnic Institute Lines: 26 NNTP-Posting-Host: wpi.wpi.edu