In article <hwbp3dc@dixie.com>, jgd@dixie.com (John De Armond) writes:
|>5916rahmank@vms.csd.mu.edu (K. M. A. Rahman) writes:
|>
|>>	Be is used in nuclear reactors, I think in shut down process.
|>
|>Nope.  That's cadmium or boron.  Be is sometimes used in 
|>sources mixed with Am-241 (called "AmBes" )as a source of neutrons
|>during reactor startup.  AmBes, sometimes with Pu replacing the Am,
|>are also used in the lab as sources of neutrons.
|>
|>>	I also heard that it's highly toxic. 
|>
|>Some compounds are.
|>
|>>What are the spectacular properties?
|>
|>Very light weight, very strong, transparent to X-rays down to very low
|>energies, good neutron moderator, excellent heat conductor, as an oxide, 
|>a very good electrical insulator while being a very good thermal 
|>conductor.  Be is the lightest metal with any structural use.
|>
|>John
|>-- 
|>John De Armond, WD4OQC               |Interested in high performance mobility?  
|>Performance Engineering Magazine (TM) |
|>Marietta, Ga                         |Interested in high tech and computers? 
|>jgd@dixie.com                        |Write me about PE Magazine
|>Need Usenet public Access in Atlanta?  Write Me for info on Dixie.com.

	Thanks for enlightening.
	May we know something about PE magazine?

	-Anis
Technical Details
Message-ID: <009618DA.1AFE29C0@vms.csd.mu.edu>
Path: arc1-ca.pugleaf.net!sparky!uunet!caen!spool.mu.edu!vms.csd.mu.edu!5916RAHMANK
References: <1992Oct2.113921.2739@mtroyal.ab.ca> <00961821.72A98CA0@vms.csd.mu.edu>,<hwbp3dc@dixie.com>

Show Full Headers
Complete Article Headers
Path: arc1-ca.pugleaf.net!sparky!uunet!caen!spool.mu.edu!vms.csd.mu.edu!5916RAHMANK
From: 5916rahmank@vms.csd.mu.edu (K. M. A. Rahman)
Newsgroups: sci.materials
Subject: Re: Uses of Be
Date: 4 Oct 1992 00:26:32 GMT
Organization: Marquette University - Computer Services
Lines: 33
Message-ID: <009618DA.1AFE29C0@vms.csd.mu.edu>
References: <1992Oct2.113921.2739@mtroyal.ab.ca> <00961821.72A98CA0@vms.csd.mu.edu>,<hwbp3dc@dixie.com>
Reply-To: 5916rahmank@vms.csd.mu.edu
NNTP-Posting-Host: vmsa.csd.mu.edu