Polysilicon: Index of Refraction vs. Temp.

#297
From: Transitive NightFall of Diamonds
Date: Mon, 21 Dec 1992 20:50
11 lines
859 bytes
I'm looking for the index of refraction for polycrystalline silicon
as a function of temperature, in the range of -100C to +50C.
If anyone knows of a reference where I can find this, please email me.

Thanks,

	Tim

----
Timothy J. Dalton                                   tjdalton@mit.edu
MIT, Dept. of Chemical Engineering, Materials Etching Technology Lab
Technical Details
Message-ID: <1992Dec21.205044.12955@athena.mit.edu>
Path: arc1-ca.pugleaf.net!sparky!uunet!enterpoop.mit.edu!bloom-picayune.mit.edu!athena.mit.edu!tjdalton

Show Full Headers
Complete Article Headers
Newsgroups: sci.materials
Path: arc1-ca.pugleaf.net!sparky!uunet!enterpoop.mit.edu!bloom-picayune.mit.edu!athena.mit.edu!tjdalton
From: tjdalton@athena.mit.edu (Transitive NightFall of Diamonds)
Subject: Polysilicon: Index of Refraction vs. Temp.
Message-ID: <1992Dec21.205044.12955@athena.mit.edu>
Followup-To: sender
Sender: news@athena.mit.edu (News system)
Nntp-Posting-Host: m66-305-1.mit.edu
Organization: Massachusetts Institute of Technology
Date: Mon, 21 Dec 1992 20:50:44 GMT
Lines: 11