In article 7602@dove.nist.gov, rochford@bldrdoc.gov (Kent Rochford 303-497-5170) writes: >I need a low loss ( loss tangent <.0005 ) RF to microwave (1MHz >to a few GHz) dielectric, preferably with a dielectric constant >around 4. Please send me any info on suppliers, vendors, or >handbooks that might help. Thanks. > >-- >Kent Rochford NIST Boulder, CO rochford@bldrdoc.gov >"No matter where you go, there you are" B. Banzai If I were you, I'd try fused silica. You can obtain this material from companies such as GE and Corning Glass Works.
Technical Details
Message-ID:
<1992Dec22.174246.22376@hubcap.clemson.edu>Path:
arc1-ca.pugleaf.net!sparky!uunet!cs.utexas.edu!sdd.hp.com!swrinde!gatech!hubcap!ellie!tdtylReferences:
<7602@dove.nist.gov>Show Full Headers
Complete Article Headers
Newsgroups: sci.materials Path: arc1-ca.pugleaf.net!sparky!uunet!cs.utexas.edu!sdd.hp.com!swrinde!gatech!hubcap!ellie!tdtyl From: tdtyl@eng.clemson.edu (Ted Taylor) Subject: Re: Looking for low-loss microwave dielectrics Message-ID: <1992Dec22.174246.22376@hubcap.clemson.edu> Sender: news@hubcap.clemson.edu (news) Reply-To: tdtyl@eng.clemson.edu Organization: College of Engineering, Clemson Univ. References: <7602@dove.nist.gov> Date: Tue, 22 Dec 1992 17:42:46 GMT Lines: 14