From: Jeff Greason ~
Date: Thu, 17 Dec 1992 19:29
Date: Thu, 17 Dec 1992 19:29
17 lines
1618 bytes
1618 bytes
In article <00965314.08C86300@vms.csd.mu.edu> 5916rahmank@vms.csd.mu.edu writes:
> Perdon my intervention. I was reading this article with interest.
> I am curious to know how the conductivity of a material is related
> to its transparency. Would you please throw some light on it?
> With thanks,
> -Anis.
In the same "hinting" tone of this thread, let me "hint" the following:
How is the conductivity of a material related to it's transparency to
radio waves? What's the difference between radio waves and light waves?
Disclaimer: All opinions expressed are my own, and do not reflect the
position of Intel, Portland State University, or Zippy the Pinhead.
============================================================================
Jeff Greason "You lock the door ... And throw away the key.
<greason@ptdcs2.intel.com> There's someone in my head, but it's not me."
<jeffg@eecs.ee.pdx.edu> -- Pink Floyd
Technical Details
Message-ID:
<1992Dec17.192957.1189@ptdcs2.intel.com>Path:
arc1-ca.pugleaf.net!sparky!uunet!usc!zaphod.mps.ohio-state.edu!saimiri.primate.wisc.edu!sdd.hp.com!spool.mu.edu!yale.edu!qt.cs.utexas.edu!cs.utexas.edu!asuvax!chnews!hfglobe!ptd!greasonReferences:
<1992Dec10.172248.28474@murdoch.acc.Virginia.EDU> <1992Dec15.100452.1@stsci.edu> <00965314.08C86300@vms.csd.mu.edu>Show Full Headers
Complete Article Headers
Newsgroups: sci.materials Path: arc1-ca.pugleaf.net!sparky!uunet!usc!zaphod.mps.ohio-state.edu!saimiri.primate.wisc.edu!sdd.hp.com!spool.mu.edu!yale.edu!qt.cs.utexas.edu!cs.utexas.edu!asuvax!chnews!hfglobe!ptd!greason From: greason@ptdcs2.intel.com (Jeff Greason ~) Subject: Re: Why some materials you can see through? Message-ID: <1992Dec17.192957.1189@ptdcs2.intel.com> Sender: news@ptdcs2.intel.com (USENET News System) Organization: Intel Corporation -- Aloha, Oregon References: <1992Dec10.172248.28474@murdoch.acc.Virginia.EDU> <1992Dec15.100452.1@stsci.edu> <00965314.08C86300@vms.csd.mu.edu> Distribution: na Date: Thu, 17 Dec 1992 19:29:57 GMT Lines: 19