Re: information wanted on cubic zirconia

#334
From: 5916rahmank
Date: Wed, 23 Dec 1992 15:27
26 lines
1537 bytes
In article <19DEC92170737@fnalh.fnal.gov> boswell@fnalh.fnal.gov writes:
>
>Hello,
>  I am working with silicon diode particle detectors, and know
>of some work with diamond, which is hard to make into a detector
>because a single crystal is more efficient, whereas the depositio
>diamond traps charge at the crystal boundaries.  This got
>me thinking:  what are the electrical properties
>of cubic zirconia, and how is it made?  If you know
>where to look, I would appreciate the info.
>
>	Chris Boswell

---------------------------------------------

	I am not too much familiar with ZrO2, but I know its electrical
	properties are complicated. Mostly it is an ionic conductor. Being
	a non-stoichiometric material, it conducts via oxygen ion transpor-
	tation. Some doped zirconia (e.g., Yittrium or Cerium doped) are
	mixed conductor and point defects (such as vacancies) play an
	important role to determine its electrical properties.

	I heard ZrO2 is used in some oxygen sensors, the ones that are
	used at higher temperatures.

	-Anis.
Technical Details
Message-ID: <0096582D.63F26140@vms.csd.mu.edu>
Path: arc1-ca.pugleaf.net!sparky!uunet!spool.mu.edu!vms.csd.mu.edu!5916RAHMANK
References: <19DEC92170737@fnalh.fnal.gov>,<Bznz6v.J87@creare.com>

Show Full Headers
Complete Article Headers
Path: arc1-ca.pugleaf.net!sparky!uunet!spool.mu.edu!vms.csd.mu.edu!5916RAHMANK
From: 5916rahmank@vms.csd.mu.edu ( )
Newsgroups: sci.materials
Subject: Re: information wanted on cubic zirconia
Date: 23 Dec 1992 15:27:20 GMT
Organization: Department of EECE, Marquette University
Lines: 26
Message-ID: <0096582D.63F26140@vms.csd.mu.edu>
References: <19DEC92170737@fnalh.fnal.gov>,<Bznz6v.J87@creare.com>
Reply-To: 5916rahmank@vms.csd.mu.edu
NNTP-Posting-Host: vmsf.csd.mu.edu