NbN is a superconductor with a Tc of 16K.

- chandra
Technical Details
Message-ID: <1992Dec24.152452.19945@noose.ecn.purdue.edu>
Path: arc1-ca.pugleaf.net!sparky!uunet!gatech!rpi!uwm.edu!spool.mu.edu!news.cs.indiana.edu!noose.ecn.purdue.edu!bank.ecn.purdue.edu!chancy
References: <1992Dec21.005356.18395@athena.mit.edu>

Show Full Headers
Complete Article Headers
Newsgroups: sci.materials
Path: arc1-ca.pugleaf.net!sparky!uunet!gatech!rpi!uwm.edu!spool.mu.edu!news.cs.indiana.edu!noose.ecn.purdue.edu!bank.ecn.purdue.edu!chancy
From: chancy@bank.ecn.purdue.edu (Venkatraman Chandrasekaran)
Subject: Re: Superconductors and Piezoelectrics
Message-ID: <1992Dec24.152452.19945@noose.ecn.purdue.edu>
Sender: news@noose.ecn.purdue.edu (USENET news)
Organization: Purdue University Engineering Computer Network
References: <1992Dec21.005356.18395@athena.mit.edu>
Date: Thu, 24 Dec 1992 15:24:52 GMT
Lines: 4