In article <1992Dec21.005356.18395@athena.mit.edu> solman@athena.mit.edu (Jason W Solinsky) writes:
>Hi all.
>
>I have a couple of questions that I was wondering if anybody here could answer.
>
>First off, I'm curious about whether NbN is a superconductor. I just saw a
>paper which said it was, and that its acoustic attenuation was dramatically
>effected by the superconducting transition, falling to zero a degrees beneath
>the Tc. I had some reason to believe that NbN was NOT a superconductor
>and I'd appreciate it if anybody here can clarify that for me.
>
... second question deleted... (i.e. I don't know)
>
>Jason W. Solinsky
According to my handy book of knowledge (CRC Chemistry and Physics
Handbook) NbN or rather NNb is a superconductor with the following
transition temperatures:
NNb (whiskers) 10-14.5 K
NNb (diffusion wires) 16.10 K
NNb (film) 6-9 K
N0.988Nb 14.9 K
N0.824-0.988Nb 14.4-15.3 K
N0.70-0.795Nb 11.3-12.9 K
Hope this helps,
Kent Goeking
Creare Inc.
kwg@spock.creare.com
Technical Details
Message-ID:
<Bzz6r0.H8z@creare.com>Path:
arc1-ca.pugleaf.net!sparky!uunet!spool.mu.edu!uwm.edu!linac!att!bu.edu!dartvax!fluent!spock!kwgReferences:
<1992Dec21.005356.18395@athena.mit.edu>Show Full Headers
Complete Article Headers
Path: arc1-ca.pugleaf.net!sparky!uunet!spool.mu.edu!uwm.edu!linac!att!bu.edu!dartvax!fluent!spock!kwg From: kwg@creare.com (Kent Goeking) Newsgroups: sci.materials Subject: Re: Superconductors and Piezoelectrics Message-ID: <Bzz6r0.H8z@creare.com> Date: 28 Dec 92 15:23:22 GMT References: <1992Dec21.005356.18395@athena.mit.edu> Reply-To: kwg@spock.creare.com (Kent Goeking) Organization: Creare Inc., Hanover, NH Lines: 31