Article #361Re: Need to make a glass surface rough ...
From: lonnie.l.houck
Date: Tue, 29 Dec 1992 15:49
Date: Tue, 29 Dec 1992 15:49
17 lines
1289 bytes
1289 bytes
In article <4rlrf7c@lynx.unm.edu> swami@chtm.eece.unm.edu (Swami srinivasan) writes: > >I need to make a 50 microns x 1000 microns section of glass surface >ROUGH. I have a mask with the required dimensions. Most etchants are >"smooth", and I suspect the common HF based etchants are, too. Are there >any wet chemical etchants that can be used? > ... other descriptions deleted ... How about generating a pattern of randomly distributed 1 micron circles of a metal on the glass. If the metal did not etch in HF or a F plasma then a very rough surface could be generated by etching the glass around these circles. With an isotropic etch and close spacing of the circles a field of random glass cones would be produced. The metal could then be stripped off and further processing could continue. Let me know whether this idea works out. Lonnie Houck llh@mvuzr.att.com
Technical Details
Message-ID:
<1992Dec29.154943.6615@cbnews.cb.att.com>Path:
arc1-ca.pugleaf.net!sparky!uunet!zaphod.mps.ohio-state.edu!pacific.mps.ohio-state.edu!linac!att!cbnews!llhReferences:
<4rlrf7c@lynx.unm.edu>Show Full Headers
Complete Article Headers
Newsgroups: sci.materials Path: arc1-ca.pugleaf.net!sparky!uunet!zaphod.mps.ohio-state.edu!pacific.mps.ohio-state.edu!linac!att!cbnews!llh From: llh@cbnews.cb.att.com (lonnie.l.houck) Subject: Re: Need to make a glass surface rough ... Organization: AT&T Distribution: usa Date: Tue, 29 Dec 1992 15:49:43 GMT Message-ID: <1992Dec29.154943.6615@cbnews.cb.att.com> References: <4rlrf7c@lynx.unm.edu> Lines: 17