In article <1993Jan4.101403.165435@dstos3.dsto.gov.au> mt_wilson@fencer.dsto.gov.au (Alan Wilson) writes:
>I have looked at Li metal in a SEM by scraping the surface while the sample
>is just out of the air lock and then quickly inserting it - probably not for
>you. I have also thought of preparing the sample under dry nitrogen and
>transferring under nitrogen into the SEM.
Not nitrogen. Li reacts with N2 to form a black film of Lithium Nitride.
The reaction is not fast, but since he's interested in the surface
conditions I would avoid nitrogen. Argon is inert toward lithium, and
is available through welding supply houses.
Sorry, I don't have any detailed suggestions about prepping for SEM.
--
--------------------------------------------------------------------------
All opinions are MINE MINE MINE, and not necessarily anyone else's.
det@phlan.sw.stratus.com | "Laddie, you'll be needin' something to wash
| that doon with."
Technical Details
Message-ID:
<1iesk8INNenk@transfer.stratus.com>Path:
arc1-ca.pugleaf.net!sparky!uunet!noc.near.net!transfer.stratus.com!phlan.sw.stratus.com!detReferences:
<BznzK5.JFH@creare.com> <1993Jan4.101403.165435@dstos3.dsto.gov.au>Show Full Headers
Complete Article Headers
Path: arc1-ca.pugleaf.net!sparky!uunet!noc.near.net!transfer.stratus.com!phlan.sw.stratus.com!det From: det@phlan.sw.stratus.com (David Toland) Newsgroups: sci.materials,sci.chem Subject: Re: SEM of lithium? Date: 6 Jan 1993 15:07:52 GMT Organization: Stratus Computer, Software Engineering Lines: 19 Message-ID: <1iesk8INNenk@transfer.stratus.com> References: <BznzK5.JFH@creare.com> <1993Jan4.101403.165435@dstos3.dsto.gov.au> NNTP-Posting-Host: phlan.sw.stratus.com