I am trying to locate fatigue crack growth data for AA2219, preferably in
the T851 temper, for the S-L orientation.  Any help would be greatly
appreciated.

RICK RATEICK
UNIVERSITY OF NOTRE DAME
RICHARD.G.RATEICK.1@ND.EDU    RRATECK@IRISHVMA.BITNET
Technical Details
Message-ID: <93027.160338RRATEICK@vma.cc.nd.edu>
Path: arc1-ca.pugleaf.net!sparky!uunet!europa.eng.gtefsd.com!emory!swrinde!zaphod.mps.ohio-state.edu!howland.reston.ans.net!spool.mu.edu!news.nd.edu!irishvma!rrateick

Show Full Headers
Complete Article Headers
Path: arc1-ca.pugleaf.net!sparky!uunet!europa.eng.gtefsd.com!emory!swrinde!zaphod.mps.ohio-state.edu!howland.reston.ans.net!spool.mu.edu!news.nd.edu!irishvma!rrateick
Date: Wednesday, 27 Jan 1993 16:03:38 EST
From: <RRATEICK@vma.cc.nd.edu>
Message-ID: <93027.160338RRATEICK@vma.cc.nd.edu>
Newsgroups: sci.materials
Subject: AA2219 aluminum crack growth rates
Lines: 7