Re: Selecting a plastic for a calculator

#423
From: gawne
Date: Wed, 27 Jan 1993 23:22
30 lines
2204 bytes
Gerald J Walsh wrote: 
>> I started by just asking people and so far, I have had Lexan or ABS
>> suggested as a possible solution.  If I choose one of those, or whatever
>> I choose for that matter, I will have to describe the crystal structure
>> (Face Center Cubic, Body Center Cubic or Hexagonal Closed Pack).  I
>> also have to discuss the market, price and my intended distribution
>> channels.  I will have to identify the materials that make up the
>> plastic I choose.  Finally, the process steps need to be discussed and
>> the companies that can provide the choosen plastic or its components.

and Kevin Weber replied: 
> Lexan or ABS are not cyrstalline, they are polymers, and while portions may
> be 'crystalline', the majority of it is not crystalline (amorphous is the
> proper term) in the sense that you are using it.  Think of them more as a
> bowl of spagetti; many long chains of atoms intertwined.

[With much more good information about polymers deleted.]

I *think* that Gerald needs information about the actual electronics of his
proposed calculator as well as the case material.  I'd guess that for a 
variety of reasons he's going to have to use Silicon (unless its for DoD,
in which case he can make it out of GaAs with a gold foil liner inside of
a radiation hardned case!).  Information about Si is available just about
anywhere, so there shouldn't be any problem finding out about the crystal
structure.

The other possibility is that whoever assigned this paper is enough of a 
goof not to know about the amorphous properties of plastics and polymers.

-Bill Gawne,  Space Telescope Science Institute
Technical Details
Message-ID: <1993Jan27.182207.1@stsci.edu>
Path: arc1-ca.pugleaf.net!sparky!uunet!math.fu-berlin.de!ira.uka.de!scsing.switch.ch!univ-lyon1.fr!ghost.dsi.unimi.it!rpi!gatech!asuvax!ncar!noao!stsci!stosc!gawne
References: <1k6fs0INNo19@elroy.jpl.nasa.gov> <weber-270193110556@129.197.66.35>

Show Full Headers
Complete Article Headers
Newsgroups: sci.materials
Path: arc1-ca.pugleaf.net!sparky!uunet!math.fu-berlin.de!ira.uka.de!scsing.switch.ch!univ-lyon1.fr!ghost.dsi.unimi.it!rpi!gatech!asuvax!ncar!noao!stsci!stosc!gawne
From: gawne@stsci.edu
Subject: Re: Selecting a plastic for a calculator
Message-ID: <1993Jan27.182207.1@stsci.edu>
Followup-To: sci.materials
Lines: 30
Sender: news@stsci.edu
Organization: Space Telescope Science Institute
References: <1k6fs0INNo19@elroy.jpl.nasa.gov> <weber-270193110556@129.197.66.35>
Distribution: na
Date: Wed, 27 Jan 1993 23:22:07 GMT