Re: Interesting friction problem

#447
From: larson eric
Date: Thu, 29 Dec 1994 19:46
23 lines
2265 bytes
DennisonC@biochem.unp.ac.za (Clive.Dennison) writes:

(A bit misdirected, but I saw this one late.)
 
>>> We are training racing thoroughbreds on high speed treadmills--fast
>>> conveyor belts with rubber surfaces. ...
>>> 
>>> The belt gradually climbs to a temperature of 100F and stops getting
>>> warmer at that point, but the shoes of the horse (steel, aluminum,
>>> titanium, and plastic shoes have been tried, as well as bare feet)
>>> continue to become hotter and hotter until, at 4 miles of 3:00 rate
>>> work, we've seen temperatures as high as 240F. this heat buildup is
>>> probably pathologic at 120F and up, since nails travel through the
>>> shoes and into the sensitive laminae of the hoof. 
===========
 
Why not mist water onto the belt?
 
-- 
Eric Larson                  | University of Illinois at Urbana-Champaign
USDA/Agronomy                | 190 PABL; 1201 W. Gregory; Urbana, IL 61801
elarson@ux1.cso.uiuc.edu     | Voice 217.244.3079  Fax 217.244.4419
Fidonet: 1:233/4.1           | My opinions are my own, but correct :-) 
Technical Details
Message-ID: <3dv3mn$565@vixen.cso.uiuc.edu>
Path: arc1-ca.pugleaf.net!nntp.gmd.de!Germany.EU.net!EU.net!howland.reston.ans.net!vixen.cso.uiuc.edu!ux1.cso.uiuc.edu!elarson
References: <3co66u$l6d@newsbf01.news.aol.com> <parkD1GGAI.7KA@netcom.com> <DennisonC.105.2F02F229@biochem.unp.ac.za>

Show Full Headers
Complete Article Headers
X-Google-Language: ENGLISH,ASCII-7-bit
X-Google-Thread: 107c0a,52ecc794ae37efc5
X-Google-Attributes: gid107c0a,public
X-Google-Thread: 1141dc,711e9de3a657a613
X-Google-Attributes: gid1141dc,public
X-Google-Thread: f665a,52ecc794ae37efc5
X-Google-Attributes: gidf665a,public
X-Google-Thread: 1086ba,52ecc794ae37efc5
X-Google-Attributes: gid1086ba,public
X-Google-Thread: 10c3c1,52ecc794ae37efc5
X-Google-Attributes: gid10c3c1,public
X-Google-Thread: 1119a6,52ecc794ae37efc5
X-Google-Attributes: gid1119a6,public
X-Google-ArrivalTime: 1994-12-29 15:27:10 PST
Path: arc1-ca.pugleaf.net!nntp.gmd.de!Germany.EU.net!EU.net!howland.reston.ans.net!vixen.cso.uiuc.edu!ux1.cso.uiuc.edu!elarson
From: elarson@ux1.cso.uiuc.edu (larson eric)
Newsgroups: sci.materials,rec.equestrian,bionet.general,sci.bio,sci.engr.biomed,sci.bio.technology,sci.bio
Subject: Re: Interesting friction problem
Date: 29 Dec 1994 19:46:31 GMT
Organization: University of Illinois at Urbana
Lines: 23
Distribution: inet
Message-ID: <3dv3mn$565@vixen.cso.uiuc.edu>
References: <3co66u$l6d@newsbf01.news.aol.com> <parkD1GGAI.7KA@netcom.com> <DennisonC.105.2F02F229@biochem.unp.ac.za>
NNTP-Posting-Host: ux1.cso.uiuc.edu