🚀 go-pugleaf

RetroBBS NetNews Server

Inspired by RockSolid Light RIP Retro Guy

Article View: sci.materials
Article #50

Re: Insulator with good heat conductivity

#50
From: jim bowers
Date: Tue, 28 Jul 1992 02:27
7 lines
660 bytes
thermal conductivity can vary quite a bit with temperature (things
generaly become much more conductive at lower temperatures).

I'm not sure there has been much research done on the thermal conductivity
of materials at very low temp.

                          Jim Bowers
Technical Details
Message-ID: <92209.222732FQV@psuvm.psu.edu>
Path: arc1-ca.pugleaf.net!sparky!uunet!dtix!darwin.sura.net!jvnc.net!rutgers!psuvax1!psuvm!fqv
References: <7926@dirac.physics.purdue.edu>

Show Full Headers
Complete Article Headers
Path: arc1-ca.pugleaf.net!sparky!uunet!dtix!darwin.sura.net!jvnc.net!rutgers!psuvax1!psuvm!fqv
From: FQV@psuvm.psu.edu (jim bowers)
Newsgroups: sci.materials
Subject: Re: Insulator with good heat conductivity
Message-ID: <92209.222732FQV@psuvm.psu.edu>
Date: 28 Jul 92 02:27:31 GMT
References: <7926@dirac.physics.purdue.edu>
Distribution: na
Organization: Penn State University
Lines: 7