Re: Insulator with good heat conductivity

#58
From: John Whitmore
Date: Wed, 29 Jul 1992 04:38
21 lines
1492 bytes
In article <7926@dirac.physics.purdue.edu> parks@gibbs.physics.purdue.edu (Chris Parks) writes:

>What is a good material (good=price + availability) which is
>an electrical insulator and a good conductor of heat?

	If your electricity is in superconductors, 'insulator' is a fair
description of copper...

>It will be used at temperatures as low as 4.2 Kelvin and it needs
>to hold up to about 200 volts / mm, heat conductivity needs to
>be comparable to copper.  Does it exist?

	Your best bet is diamond, but you've already ruled that 
out (why, I can't imagine...).  Do you honestly want comparable
heat conductivity at 4.2K to the conductivity of copper at 4.2K?
Thermal conductivity of Cu is about 4W/cm/K at room temperature,
but 113W/cm/K at helium temperature.  Except for diamond, your
best bet is BeO (highly toxic, by the way!) but the only data I have
is for higher temperatures (125 BTU-in/hr/sq. ft/F).

	John Whitmore
Technical Details
Message-ID: <1992Jul29.043801.21860@u.washington.edu>
Path: arc1-ca.pugleaf.net!sparky!uunet!zaphod.mps.ohio-state.edu!uakari.primate.wisc.edu!usenet.coe.montana.edu!news.u.washington.edu!milton.u.washington.edu!whit
References: <7926@dirac.physics.purdue.edu>

Show Full Headers
Complete Article Headers
Path: arc1-ca.pugleaf.net!sparky!uunet!zaphod.mps.ohio-state.edu!uakari.primate.wisc.edu!usenet.coe.montana.edu!news.u.washington.edu!milton.u.washington.edu!whit
From: whit@milton.u.washington.edu (John Whitmore)
Newsgroups: sci.materials
Subject: Re: Insulator with good heat conductivity
Message-ID: <1992Jul29.043801.21860@u.washington.edu>
Date: 29 Jul 92 04:38:01 GMT
References: <7926@dirac.physics.purdue.edu>
Sender: news@u.washington.edu (USENET News System)
Distribution: na
Organization: University of Washington, Seattle
Lines: 21