Re: Solvent for PVDF

#79
From: Tom Knight
Date: Fri, 31 Jul 1992 21:35
8 lines
866 bytes
  (Timothy J. Drabik) writes:
  I'm looking for a solvent for polyvinylidene flouride.
   I would like to spin-deposit it.  Can anyone recommend
   a journal reference or a chemical?

Perhaps it would be possible to spin the monomer and polymerize it in situ.
The down side is that the monomer is probably incredibly toxic.
Technical Details
Message-ID: <TK.92Jul31173523@wheat-chex.ai.mit.edu>
Path: arc1-ca.pugleaf.net!sparky!uunet!usc!wupost!gumby!yale!mintaka.lcs.mit.edu!ai-lab!life!tk
References: <1992Jul30.170903.12107@ee.gatech.edu> <1992Jul31.175332.10341@kodak.kodak.com>

Show Full Headers
Complete Article Headers
Path: arc1-ca.pugleaf.net!sparky!uunet!usc!wupost!gumby!yale!mintaka.lcs.mit.edu!ai-lab!life!tk
From: tk@ai.mit.edu (Tom Knight)
Newsgroups: sci.materials
Subject: Re: Solvent for PVDF
Message-ID: <TK.92Jul31173523@wheat-chex.ai.mit.edu>
Date: 31 Jul 92 21:35:23 GMT
References: <1992Jul30.170903.12107@ee.gatech.edu>
 <1992Jul31.175332.10341@kodak.kodak.com>
Sender: news@ai.mit.edu
Followup-To: sci.materials
Organization: MIT Artificial Intelligence Lab
Lines: 8
In-reply-to: ornitz@kodak.kodak.com's message of 31 Jul 92 17:53:32 GMT