In article <1992Aug4.014634.10230@msuinfo.cl.msu.edu> delgado@robin.egr.msu.edu 
(Richard Delgado) writes:
>
>I have been searching for polymer dielectric data over the microwave frequency 
>range and 
>over any temperature range. I would appreciate any input. There doesn't seem to
>be much (
>or for that matter, any ) of this type of data published.

Call me at the number below; I think I can be of help.  From experience I can
say that there are very few applications of microwave processing that cannot
be done less expensively by means of other methods.  The heating of extremely
high viscosity polymers is one of them.

BTW, please learn to format your postings to a maximum of 80 columns.

				Barry
 -----------------
|  ___  ________  |       Dr. Barry L. Ornitz          WA4VZQ
| |  / /        | |       Eastman Kodak Company
| | / /         | |       Eastman Chemical Company Research Laboratories
| |< < K O D A K| |       Process Instrumentation Research Laboratory
| | \ \         | |       P. O. Box 1972, Building 167B
| |__\ \________| |       Kingsport, TN  37662       615/229-4904
|                 |       INTERNET:   ornitz@kodak.com
 -----------------
Technical Details
Message-ID: <1992Aug4.214916.16468@kodak.kodak.com>
Path: arc1-ca.pugleaf.net!sparky!uunet!zaphod.mps.ohio-state.edu!rpi!newsserver.pixel.kodak.com!kodak!ornitz
References: <1992Aug4.014634.10230@msuinfo.cl.msu.edu>

Show Full Headers
Complete Article Headers
Newsgroups: sci.materials
Path: arc1-ca.pugleaf.net!sparky!uunet!zaphod.mps.ohio-state.edu!rpi!newsserver.pixel.kodak.com!kodak!ornitz
From: ornitz@kodak.kodak.com (Barry Ornitz)
Subject: Re: Microwave Processing of Polymers
Message-ID: <1992Aug4.214916.16468@kodak.kodak.com>
Followup-To: sci.materials
Sender: Barry L. Ornitz
Organization: Eastman Kodak Company, Eastman Chemical Company Research Labs
References: <1992Aug4.014634.10230@msuinfo.cl.msu.edu>
Distribution: na
Date: Tue, 4 Aug 92 21:49:16 GMT
Lines: 27