Re: Superconducting Gallium Arsenide... what's the latest?

#92
From: Chris Parks
Date: Thu, 06 Aug 1992 22:48
13 lines
1104 bytes
In article <zyxm4pb@lynx.unm.edu> swami@chtm.eece.unm.edu (Swami srinivasan) writes:
>
>A few months back, there was talk about superconductivity in GaAs with
>Arsenic precipitates. As far as i can recall, Tc was below 30 K.
>		Danke Sehr!

It is my understanding that the original claim published in
Phys. Rev. Lett. was bogus.  The reason for it was explained to me
long ago and I've since forgotten.  I'd also be interested in the
reason if anyone knows. 

Chris Parks
parks@physics.purdue.edu
Technical Details
Message-ID: <8018@dirac.physics.purdue.edu>
Path: arc1-ca.pugleaf.net!sparky!uunet!zephyr.ens.tek.com!uw-beaver!ubc-cs!destroyer!caen!uakari.primate.wisc.edu!ames!purdue!mentor.cc.purdue.edu!noose.ecn.purdue.edu!dirac!gibbs.physics.purdue.edu!parks
References: <zyxm4pb@lynx.unm.edu>

Show Full Headers
Complete Article Headers
Path: arc1-ca.pugleaf.net!sparky!uunet!zephyr.ens.tek.com!uw-beaver!ubc-cs!destroyer!caen!uakari.primate.wisc.edu!ames!purdue!mentor.cc.purdue.edu!noose.ecn.purdue.edu!dirac!gibbs.physics.purdue.edu!parks
From: parks@gibbs.physics.purdue.edu (Chris Parks)
Newsgroups: sci.materials
Subject: Re: Superconducting Gallium Arsenide... what's the latest?
Keywords: As precipitates, superconductivity
Message-ID: <8018@dirac.physics.purdue.edu>
Date: 6 Aug 92 22:48:55 GMT
References: <zyxm4pb@lynx.unm.edu>
Sender: news@dirac.physics.purdue.edu
Organization: Purdue University Physics Department
Lines: 13