1 total messages Started by Dale E. Alexander Mon, 10 Aug 1992 20:44
isotope availability
#104
Author: Dale E. Alexander
Date: Mon, 10 Aug 1992 20:44
8 lines
1000 bytes
I'm in need of stable isotopic Cu (Cu-63 & Cu-65) for use in a thin film
evaporator.  We're preparing a multilayer strucuture in which we will use
small angle neutron diffraction as a sensitive technique for studying
interdiffusion.  Ideally I need about 2 g of each with isotopic purities of
>90%.  Oak Ridge is the only source I'm aware of in the States.  Does
anyone have a connection with the Former Soviet Union.  I'm hoping such
things are available (at less than $4/mg price ORNL charges) from our new
allies.  Any leads?
Thread Navigation

This is a paginated view of messages in the thread with full content displayed inline.

Messages are displayed in chronological order, with the original post highlighted in green.

Use pagination controls to navigate through all messages in large threads.

Back to All Threads