2 total messages Started by Adam Karpowicz Mon, 13 Apr 1992 00:40
Re: carbon fibre bows
#138
Author: Adam Karpowicz
Date: Mon, 13 Apr 1992 00:40
8 lines
595 bytes
I want to thank everyone who responded to my questions on
carbon/graphite composites, the discussion that followed was
enlightening.

I still do not know what is carbon foam.    

Adam
Re: steel foam
#139
Author: Marvin Minsky
Date: Mon, 13 Apr 1992 02:12
21 lines
1499 bytes
In article <1992Apr13.004026.2744@jupiter.sun.csd.unb.ca> akarpowicz@mta.ca writes:
>
>I want to thank everyone who responded to my questions on
>carbon/graphite composites, the discussion that followed was
>enlightening.
>
>I still do not know what is carbon foam.    
>
>Adam

Either do I, but that reminds me of an question I've had for a long
time: why isn't there a structural steel foam material?  Seems to me
it should be very strong and cheap, if there's a good way to make it.
Is the problem simply one of how to keep bubbles from rising?
Clearly, zero-gee ought to help, but I would suppose someone could
invent some way to make such a material!  One way would be to inject
bubbles at high pressure when the steel is at a viscous temperature,
and then rotate it while it does the remaining cooling.  Once the
outside of the "ingot" hardens, we don't care much that the pressure
inside goes negative; in fact that could be an advantage.
  Other ideas might include using some sort of refactory mesh to hold
Thread Navigation

This is a paginated view of messages in the thread with full content displayed inline.

Messages are displayed in chronological order, with the original post highlighted in green.

Use pagination controls to navigate through all messages in large threads.

Back to All Threads