SUMMARY: Electro-Rheology materials
#143
Author: douglas.w.monroe
Date: Mon, 13 Apr 1992 16:29
148 lines
5899 bytes
A week or so ago I posted a request for info regarding
electro-rheological materials. Below is my original posting and the
collection of responses. Thanks to *all* who responded! There
seemed to be sufficient interest from other wanting info to warrant
this summary. Hope it helps someone.

Original Posting:

 Hi there! A long time back, I recall reading about a material(s?) 
which change from solid to liquid-like upon application of voltage. 
I believe this was used in a clutch or braking application. If I 
remember correctly, the material was refered to as an electro-
rheological fluid. Anyone have any details about these materials and 
whether they are commercially available? Please e-mail,
 I'll sumarize if there's enough interest.



Responses follow:

From: boland@cps.msu.edu

 
There was a Prof. Filisko at the UM-Ann Arbor who patented what you are
referring to (I think).  This must have been 5 years ago or so... One
of the automakers were looking into applications I think.  I'm sure
you could do a journal search...  Hope this helps...
 
jb
*************************************************************

From: jrtyner@eos.ncsu.edu


   Our Dr. Conrad and some students and co-workers have been working on ER
fluids.  I don't know details, but he may be reached at 
      
      NCSU
      Dept. of Materials Science and Engineering
      Box 7907
      Raleigh, NC  27695-7907

      (919) 515-2377  			


John
**************************************************************

From: J. A. Sarreal <sarreal@mcnc.org>

I believe the pioneer for this type of material is Dr. Conrad
at NCSU.  You may want to correspond with him about this.

The Dept. of Mat. Sci. and Eng. #: 919-737-2377

GOOD LUCK!    
************************************************************

From: hiro@ccwf.cc.utexas.edu (Hiro)

ER fluids consist of two mail ingredients: the base liquid and the
suspended particles. The base liquid must be a good electrical insulator
and strongly hydrophobic. The spherical particles (zeolites), ranging from
submicron to several microns in diameter is porous and make up 15-40% of
the liquid. The physical reason for the properties of ER fluids is not
well understood, but apparently, the absorption/desorption of the liquid
into/out of the zeolite is a key factor.

I did a senior project on designing a brake using ER fluid 3yrs ago, and I
have the following references:

1. W. M. Winslow, J. Appl. Phys. vol. 20, (1949).
2. J. E. Strangroom, Phys. Technol, vol. 14 6(1983).
3. F. Zukoski, and J. W. Goodwin, Proc. IECON 1986 Industrial Application of 
   Mini, Micro & Personal computers, vol. 1 (1986).
4. Engineering vol.228, pp.i-iv (1988).
5. A. F. Sprecher, J. d. Carson, and H. Conrad, Mat. Sci. and Eng. vol. 95 
   (1987).
6. N. G. Stevens, J. L. Sproston and R. Stanway, J. Electrostatics, vol. 17 
   (1985).

I wrote the paper in 1989, so are probably more recent papers. Also, there
is extensive research being done in England. The following companies have ER 
fluids for sale:

ER Fluid Developments, London
British Technology Group
Castrol Corp.
Lord Corp, North Carolina

I hope the above information will get you started. Also, I would be very 
interested in learning about your research and application of ER fluids.

Hiro Kinoshita
----------------------------------------------------------------------------
hiro@ccwf.cc.utexas.edu
Microelectronics Research Center
Department of Electrical and Computer Engineering
The University of Texas at Austin
Austin, TX 

*****************************************************************

From: Joe Rosato <jarj_ss@uhura.cc.rochester.edu>

Here are some references on Electrorheological Fluids.
Hope they help.

Klass Donald L. & Martinek, Thomas W., 1967
"Electroviscous Fluids. I. & II Rheological Properties"
Journal of Applied Physics, 38(1) p.67-80

Stevens, N.G., Sproston, J.L., Stanway, R., 1985
"The Influence of Pulsed D.C. Input signals on Electrorheological fluids"
Journal of Electrostatics, 17 p.181-191

Stevens, N.G., Sproston, J.L., Stanway, R., June 1988
"An Experimental Study of Electrorheological Torque Transmission"
Journal of Mechanisms, Transmissions, and Automation in Design, 110 p.182-188

Pool, Robert, March 1990
"The Fluids with a case of Split Personality"
Science 24 p.1180-1181

Webb, Nigel, April 1990
"Electrorheological fluids"
Chemestry in Britain, p.338-340

Goldstein, Gina, Oct 1990
"Electrorheological fluids: Applications begin to gel"
Mechanical Engineering  p.48-52

					
****************************************************************
From: routd@woods.ulowell.edu

hi doug,
this is interesting! I want to know more about them. I can guess something
like this: if a polymer is having anisotropy, or liquid crystallinity, say, lcp
like vectra and kevlar. one can orient the molecules(again assuming that there is a substantial dipole moment associated) in e-field and thus changing the tensile strength drastically( tensile strength is also anisotropic)
Thanks and hope to hear from u soon!
********************************END*******************************
-- 
******************************************************************************
                                                          Doug Monroe
                   				       dwm@pruxl.att.com
  						 -or-  monwel@cbnewsk.att.com
Thread Navigation

This is a paginated view of messages in the thread with full content displayed inline.

Messages are displayed in chronological order, with the original post highlighted in green.

Use pagination controls to navigate through all messages in large threads.

Back to All Threads