	Hello there. I'm a fourth-year undergrad (read: lab peon) and I was
curious to know what methods people know of for attaching .001 wire to samples
of YBCO superconductor. It's been a bit troublesome, and I'm curious just to
hear what people have to say on the subject.


-- 
*	Adrian "Nick" Marden  	    *	"The A's have Dennis Eckersley-	      *
*	mard@quads.uchicago.edu     *	he doesn't blow anyone!"	      *
*	home:(312)-684-1913	    *			-Steve Stone	      *
*	work(?):(312)-702-7269	    *					      *
Thread Navigation

This is a paginated view of messages in the thread with full content displayed inline.

Messages are displayed in chronological order, with the original post highlighted in green.

Use pagination controls to navigate through all messages in large threads.

Back to All Threads