I saw an article in NASA Tech. Briefs (Aug 92) about some work being done to monitor the cure state of composite resins using electromagnetic imaging. This looks like it may have application to one area of work here. Unfortunately, the article indicates that no further information is available. Can someone point me to 1) references by the authors below or 2) e-mail or phone addresses of any one of the authors so I can get additional information? "Monitoring Polymer Curing via Electromagnetic Impedance", NASA Tech. Briefs, Aug 92, William Freeman and John C. Covington @ NASA Langley and David Kranbuehl, Melanie Hoff, and Susan Delo? at College of William and Mary. Jim L. Novak Intelligent System Sensors and Controls Sandia National Laboratories (505) 844-4227 jlnovak@isrc.sandia.gov
Thread Navigation
This is a paginated view of messages in the thread with full content displayed inline.
Messages are displayed in chronological order, with the original post highlighted in green.
Use pagination controls to navigate through all messages in large threads.
Back to All Threads