Gentlemen,
Sub : Reg. Position as Materials Scientist.
I have been working as a Metallurgist and Materials Scientist
for the past 17 years. I would like to put to use my acquired knowledge
and skills in these fields of research in a practical way. I am keen to
work in interdisciplinary areas of research.As you can make out from my
cv and the list of my publications, I have sufficient expertise in
materials development as well as testing and evaluation. I have been
involved in several research projects in the above fields. I also have
some basic knowledge about ceramics and composites. Currently, I am on
sabbatical leave, for the purpose of pursuing Post-Doctoral Research.
Please respond by e-mail to the address shown below, if you can offer
me a research position in your organisation.
Yours sincerely,
S. Venkadesan
Department of Mechanical and Materials Engineering
University of Western Australia
Nedlands, 6009, WA.
E-mail :venky@shiralee.mech.uwa.edu.au
venky@uniwa.uwa.edu.au
=============================================================================
CURRICULUM-VITAE
1. Name : SRINIVASAN VENKADESAN.
2. Date & Place of Birth : 2-6-1951, Mathura (U.P) India.
3. Permanent Address : No 17, 4th Street, KALPAKKAM - 603 102.
INDIA.
4. Present Address : Dept. Mechanical and Materials Engineering,
University of Western Australia,
Nedlands, WA 6009
Western Australia.
Phone : (09) 380 3132. Fax :(09) 380 1024
E-mail: venky@shiralee.mech.uwa.edu.au
venky@uniwa.uwa.edu.au
5. Educational Qualifications :
a) B.Sc. (Physics) Madurai University, Tuticorin, 1971.
b) B.E. (Metallurgy) Indian Institute of Science, Bangalore, 1974.
c) M.S. (Metallurgy) Indian Institute of Technology, Madras,1982.
d) Ph.D. (Metallurgy) Indian Institute of Technology, Madras, 1991.
6. Professional Experience :
a) Trainee BARC, 1974-75. BARC, Bombay- 400 085
Training INDIA.
School
b) Scientific Materials 1975-86. IGCAR, Kalpakkam- 603 102.
Officer Development INDIA.
Laboratory,
c) Section Materials 1986-92. IGCAR, Kalpakkam- 603 102.
Head Technology INDIA.
Section,
d)Gledden Dept.Mech. .From Univ. of Western Australia,
Senior &Mater Aug.92 Nedlands, WA 6009,
Visiting Engg. Western Australia
Fellow
7. Participation in summer schools, short-term courses etc. :
a) Continuing Education Programme on High Energy Rate Forming Techniques
held at Ind.Inst.Technol., Madras, India.1976.
b) Special Lectures on Metal Forming Tools conducted by
Prof.Dr.Ing.H.W.Wagner at Ind.Inst.Technol., Madras, India.1983.
c) Spring College in Materials Science on Ceramics and Composite
Materials held at ICTP, Trieste, Italy.1989.
d) Working Party on Modelling Thermomechanical Behaviour of Materials
held at ICTP, Trieste, Italy.1989.
8. Fields of Research Interest :
Phase Transformations, Microstructure - Mechanical Properties Correlation,
Metal Forming, Welding, Alloy Development, Deformation Mechanisms, Dynamic
Strain Ageing and Ceramics.
9) Skills in experimental techniques:
Scanning Electron Microscopy, Electron Probe Microanalysis, Transmission
Electron Microscopy, Vacuum melting and heat treatment, Metal forming
operations such as forging, rolling, press working, wire drawing and extrusion,
Mechanical testing in tension, torsion and compression, Data analysis related
to all the above experimental techniques
10. List of Publications of S. VENKADESAN
a) Publications in Journals
1)The Influence of Post-Weld Heat Treatment on the Structure, Composition
and the Amount of Ferrite in Type 316 Austenitic Stainless Steel Welds.
V. S. RAGHUNATHAN, V. SEETHARAMAN, S. VENKADESAN and P. RODRIGUEZ.
Metall. Trans. A, Vol. 10 A, pp. 1683-1689, 1979.
2) Strain-Temperature Correlations Obtained in Rolling.
A. P. SINGH, S. VENKADESAN and K. A. PADMANABHAN.
Mater. Sci. Engg., Vol. 58, pp. 223-227, 1983.
3) Tensile Deformation Behaviour of Warm-Rolled Type 316 Austenitic
Stainless Steel.
S. VENKADESAN, P. V. SIVAPRASAD, S. VENUGOPAL and V. SEETHARAMAN.
Jl. Mech. Work. Technol., Vol. 12, pp. 351-366, 1986.
4) Applicability of Ludwigson's Equation for Describing the Tensile Flow
Behaviour of Warm- Rolled Type 316 Stainless Steel.
P. V. SIVAPRASAD, S. VENKADESAN, S. VENUGOPAL and V. SEETHARAMAN.
Scripta Metall., Vol. 20, pp. 603-604, 1986.
5) Investigation of the Strength Retention of a Warm-Rolled Austenitic
Stainless Steel Through Hot-Hardness Measurements.
S. VENKADESAN, G. VENKATARAMAN and V. SEETHARAMAN.
Jl. Mech. Work. Technol., Vol. 15, pp. 81-89, 1987.
6) On the Warm Rolling of Type 316 Austenitic Stainless Steel.
S. VENKADESAN and K. A. PADMANABHAN.
Z. Metallkde., Vol. 79, pp. 174-179, 1988.
7) Analysis of Tensile Work Hardening Behaviour of Warm Worked Type 316
Austenitic Stainless Steel.
S. VENKADESAN, P. V. SIVAPRASAD, S. K. RAY and V. SEETHARAMAN.
Z. Metallkde., Vol. 79, pp. 226-230, 1988.
8) Development of Transition Metal Joint for Steam Generator Circuit of
Prototype Fast Breeder Reactor.
A. K. BHADURI, I. GOWRISANKAR, V. SEETHARAMAN, S. VENKADESAN and P. RODRIGUEZ.
Mater. Sci. Technol., Vol. 4, pp. 1020-1029, 1988.
9) Computer Simulation of Isotherms in the Heat-Affected Zone During Bead-
on-Plate Welding.
A. K. BHADURI, V. SEETHARAMAN and S. VENKADESAN.
Trans. Ind. Inst. Metals, Vol. 41, pp. 481-484, 1988.
10) An Examination of the Relative Merits of the Compression Test and the
Torsion Tests for the Prediction of Peak Pressures During the Extrusion of
Commercial Purity Titanium.
S. VENUGOPAL, G. SRINIVASAN, S. VENKADESAN, V. SEETHARAMAN and P. VENUGOPAL.
Jl. Mech. Work. Technol., Vol. 19, pp. 151-163, 1989.
11) A Note on the Determination of the Friction Factor by Means of the
Reduction-Capacity Test.
S. VENUGOPAL, G. SRINIVASAN, S. VENKADESAN and V. SEETHARAMAN.
Jl. Mech. Work. Technol., Vol. 19, pp. 261-266, 1989.
12) Effect of Ageing on the Interfacial Microstructure and Mechanical
Properties of a Alloy 800 / 2. 25 Cr-1 Mo Steel Joint.
A. K. BHADURI, V. SEETHARAMAN and S. VENKADESAN.
Z. Metallkde., Vol. 80, pp. 630-634, 1989.
13) Microstructure of the Heat Affected Zone in 17-4 PH Stainless Steel.
A. K. BHADURI and S. VENKADESAN.
Steel Research, Vol. 60, pp. 509-513, 1989.
14) Surface Area and Pore Size Studies of Alumina Gels.
G. V. RAMA RAO, V. SARASWATI and S. VENKADESAN.
Jl. Non-Cryst. Solids, Vol. 111, pp. 103-112, 1989.
15)Development of Cladding and Structural Materials for Thermal and Fast
Reactor Programme in India.
C. V. SUNDARAM, P. RODRIGUEZ, S. L. MANNAN and S. VENKADESAN.
Mater. Sci. Forum, Vol. 48 & 49, pp. 21-48, 1989.
16) Intergranular Corrosion Studies on Warm Worked Type 316 Austenitic
Stainless Steel.
U. KAMACHI MUDALI, S. VENKADESAN and J. B. GNANAMOORTHY.
Jl. Mater. Engg., Vol. 12, No. 3, pp. 227-234, 1990.
17) Effect of Thermal Cycling on the Alloy 800/2. 25Cr-1Mo Steel Joint.
A. K. BHADURI and S. VENKADESAN.
Z. Metallkde., Vol. 82, No. 2, pp. 135-138, 1991.
18) Combined Effect of Post Weld Heat Treatment and Ageing on the Alloy 800/
2.25Cr-1Mo Steel Joint.
A. K. BHADURI, S. VENKADESAN, P. RODRIGUEZ and P. G. MUKUNDA.
Mater. Sci. Technol., Vol. 7, pp. 1051-1056, 1991.
19) Effect of Ageing on the Microstructural Stability of Cold Worked Titanium
Modified 15Cr-15Ni-2. 5Mo Austenitic Stainless Steel.
S. VENKADESAN, A. K. BHADURI, P. RODRIGUEZ and K. A. PADMANABHAN.
Jl. Nucl. Mater., Vol. 186, pp. 177-184, 1992.
20) Activation Energy for Serrated Flow in a 15Cr-15Ni Ti- Modified
Austenitic Stainless Steel.
S. VENKADESAN, C. PHANIRAJ, P. V. SIVAPRASAD and P. RODRIGUEZ.
Acta Metall. Mater., Vol. 40, pp. 569-580, 1992.
21) Effect of Ti/C Ratio and Prior Cold Work on the Tensile Properties of
15Cr-15Ni-2. 2Mo Titanium Modified Austenitic Stainless Steel.
S. VENKADESAN, P. V. SIVAPRASAD, M. VASUDEVAN, S. VENUGOPAL and P. RODRIGUEZ.
Trans. Ind. Inst. Metals, Vol. 45, No. 1, pp. 57-68, 1992.
22) A Note on the Predominance of Dynamic Strain Ageing over the Adiabatic
Shear Deformation Phenomenon in Commercial Purity Titanium in Compression tests
at Strain Rates of 0. 05 to 32 s-1and Temperatures of 303 to 573 K.
S. VENUGOPAL, S. VENKADESAN, S. L. MANNAN and P. VENUGOPAL.
Jl. Mater. Process. Technol., Vol. 30, pp. 245-251, 1992.
23) Flow Transients During Strain Rate Jump Tests in a Titanium Modified
Austenitic Stainless Steel.
S. VENKADESAN, P. RODRIGUEZ, K. A. PADMANABHAN, P. V. SIVAPRASAD and
C. PHANIRAJ.
Mater. Sci. Engg., Vol. A 154, pp. 69-74, 1992.
24) Performance of a Trimetallic Transition Joint.
A. K. BHADURI, S. VENKADESAN, P. RODRIGUEZ and P. G. MUKUNDA.
Mater. at High Temps., (in Press) 1992.
25) Influence of Temperature and Strain Rate on the Tensile Properties of a
15Cr-15Ni-2. 2Mo- Ti Modified Austenitic Stainless Steel.
S. VENKADESAN, S. VENUGOPAL, M. VASUDEVAN and P. V. SIVAPRASAD.
Mater. Sci. Technol., (in Press) 1992.
26) Flow Localization Behaviour of AISI 304L Austenitic Stainless Steel in
Warm and Hot Working Regions.
M. VASUDEVAN, S. VENUGOPAL, S. VENKADESAN and S. L. MANNAN.
Mater. Sci. Technol., (in Press)1992.
27) Role of Strain Induced Vacancies in Serrated Flow.
S. VENKADESAN, P. V. SIVAPRASAD, C. PHANIRAJ and P. RODRIGUEZ.
Z. Metallkde., (in Press)1992.
28) Geometric Representation of Equivalent Strain and Some Applications to
Sheet Metal Forming.
C. RAVISHANKAR, S. VENKADESAN and P. RODRIGUEZ.
Communicated to Jl. Mater. Shaping Technol., 1992.
29) The Effect of Diffusion Barrier Formation on the Kinetics of Aluminizing
in Inconel-718.
V. SHANKAR, J. ANNAPURNA, A. L. E. TERRANCE and S. VENKADESAN.
Communicated to Mater. Sci. Engg., 1992.
30) Stress Corrosion Cracking of 15Cr-15Ni-2. 2 Mo Titanium Modified
Austenitic Stainless Steel.
HASAN SHAIKH, S. VENKADESAN, C. NARAYANAN, H. S. KHATAK and J. B. GNANAMOORTHY.
Communicated to Jl. Mater. Engg. & Perf., 1992.
31) Influence of Temperature and Strain Rate on the Nature of Serrations
Observed During Tensile Testing.
S. VENKADESAN, S. VENUGOPAL, P. V. SIVAPRASAD and P. RODRIGUEZ.
Communicated to Trans. Jap. Inst. Metals, 1992.
b) Publications in Proceedings of Conference, Seminar etc. :
1)Microstructural Stability of Type 316 Stainless Steel Welds.
S. VENKADESAN, V. SEETHARAMAN, V. S. RAGHUNATHAN and P. RODRIGUEZ.
Proc. Afro-Asian Conf. on Welding and Metals Technology, New Delhi, Feb. 1978.
2) Time-Temperature-Sensitisation Diagram for Type 316 Stainless Steel
with Different Degrees of Cold Work and Its Use for Continuous Cooling/
Heating Treating.
R. K. DAYAL, N. PARVATHAVARDHINI, S. VENKADESAN, S. K. MANNAN and
J. B. GNANAMOORTHY.
Proc. Workshop on Experience and Use of Stainless Steel Equipment in
Department of Atomic Energy Projects, Vol. III, paper C-66, Kalpakkam,
Mar 1981.
3) Warm Working of Austenitic Stainless Steels.
S. VENKADESAN, V. SEETHARAMAN and K. A. PADMANABHAN.
Proc. Natl. Sem. on Stainless Steels in the 80s, Salem, Dec. 1982, pp. 51-56,
1982.
4) Assessment of Lubricants for Forming of Armco Iron and Titanium.
S. VENUGOPAL, V. SEETHARAMAN and S. VENKADESAN.
Proc. Natl. Sem. on Modern Trends in Metal Forming Techniques, Instn. of Engrs.
(India), Nov. 1986, Hyderabad, pp 3. 115-3. 124, 1986.
5) Warm Working - Basis, Profits and Problems : An Analysis with Respect to
Austenitic Stainless Steels.
S. VENKADESAN, V. SEETHARAMAN and P. RODRIGUEZ.
- ibid, pp. 2. 67-2. 78, 1986.
6) Effect of Post-Weld Heat Treatment on the Mechanical Properties of the
Dissimilar Metal Joint Between Alloy 800 and 2. 25Cr-1Mo Steel Made with
Inconel 182 Electrode.
A. K. BHADURI, V. SEETHARAMAN and S. VENKADESAN.
Proc. Internl. Welding Conf. - IWC-87, Jan. 1987, New Delhi, pp. 545- 560, 1987.
7) Effect of Welding Parameters on the Microstructure of Stellite -6
Deposits.
S. K. ALBERT, I. GOWRISHANKAR, V. SEETHARAMAN and S. VENKADESAN.
Proc. Natl. Welding Sem. NWS-87, Nov. 1987, pp. A1-A7, 1987.
8) Heat Treatment of Austenitic Stainless Steel Components.
R. K. DAYAL, S. VENKADESAN and J. B. GNANAMOORTHY.
Proc. Sem. on Heat Treatment, Ind. Inst. Technol., Madras, Oct. 1987, pp. 15-29,
1987.
9) Electro-Slag Welding of AISI Type 316 Stainless Steel.
S. VENUGOPAL, V. SEETHARAMAN, S. VENKADESAN, P. RODRIGUEZ, B. RADHAKRISHNAN,
M. A. PARAMESWARA, B. DWARAKANATH RAO and V. RAMACHANDRAN.
Proc. Natl. Welding Sem. NWS-88, Ind. Inst. Welding, Cochin, Nov. 1988,
pp. R9/1-R9/9, 1988.
10) Development of Low Swelling Austenitic Stainless Steel for In- core
Applications of Prototype Fast Breeder Reactor.
S. VENKADESAN, P. V. SIVAPRASAD, C. NARAYANAN and V. SHANMUGAM.
Proc. Internatl. Conf. on Stainless Steels INCOSS-89, Ind. Inst. Metals,
Bombay, Feb. 1989. (Eds. P. Krishna Rao et al. ), Omega Scientific
Publishers, New Delhi, 1992, pp. 345-360, 1992.
11) Stainless Steel Application in Prototype Fast Breeder Reactor.
S. C. CHETAL, S. B. BHOJE, S. GOVINDRAJAN, S. L. MANNAN, S. R. PARANJPE,
P. RODRIGUEZ and S. VENKADESAN.
- ibid, pp. 361-373.
12) Development of Cladding and Structural Materials for Thermal and Fast
Reactor Programme in India.
C. V. SUNDARAM, P. RODRIGUEZ, S. L. MANNAN and S. VENKADESAN.
Proc. Symp. on Nuclear Fuel Fabrication NUFAB-88, Board of Research in Nuclear
Sciences, Bombay, Dec. 1988. pp. 21-48, 1989.
13) Microstructure, Mechanical Property and Performance Simulation of Alloy
800/ 2. 25 Cr-1Mo Steel Joint.
A. K. BHADURI, S. VENKADESAN and P. RODRIGUEZ.
Proc. Natl. Welding Sem. NWS-89, Ind. Inst. Welding, New Delhi, Dec. 1989,
pp. 4. 1-4. 10, 1989.
14) Microstructural Stability of Cold Worked Titanium Modified Austenitic
Stainless Steel.
S. VENKADESAN, A. K. BHADURI and P. RODRIGUEZ.
Proc. Internl. Conf. on Fast Reactor Core and Fuel Structural Behavior, BNES,
Inverness, U. K. June 1990, Paper No : 44, pp. 249-254, 1990.
15) Development and Characterization of Materials for Prototype Fast Breeder
Reactor.
P. RODRIGUEZ, S. L. MANNAN, S. VENKADESAN and K. B. S. RAO.
Proc. Internl. Conf. on Fast Reactors and Related Fuel Cycles (FR'91), Kyoto,
Japan, Atomic Energy Society of Japan, Tokyo, Japan, Oct 28-Nov 1, 1991,
Paper No : 7-3.
16) Studies on Nickel Base Hard-Facing Alloy Deposited on SS.
S. K. ALBERT, S. VENKADESAN and S. L. MANNAN.
Proc. Sem. on Joining of Metals (SOJOM 91), Ind. Inst. Welding, Trichy, India.
Dec 12-14, 1991, Paper No : B14, pp. 363- 369, 1991.
c) Thesis Reports Submitted :
1)Construction of a Pressure Infiltration Equipment for the Production of
Composites.
S. VENKADESAN.
B. E. Project Thesis, Ind. Inst. Science., Bangalore. Apr. 1974.
2) An Investigation on the Warm Rolling of An Austenitic Stainless Steel.
S. VENKADESAN.
M. S. Thesis, Ind. Inst. Technol., Madras. Aug. 1982.
3) Development and Characterization of the Tensile Deformation Behaviour of
A Titanium Modified Austenitic Stainless Steel.
S. VENKADESAN.
Ph. D. Thesis, Ind. Inst. Technol., Madras. Apr. 1991.
Thread Navigation
This is a paginated view of messages in the thread with full content displayed inline.
Messages are displayed in chronological order, with the original post highlighted in green.
Use pagination controls to navigate through all messages in large threads.
Back to All Threads