Article View: comp.robotics
Article #811Re: Nitinol message
From: Dan Liddell
Date: Mon, 19 Nov 1990 17:40
Date: Mon, 19 Nov 1990 17:40
11 lines
933 bytes
933 bytes
I have seen ohmic heating used as a method of providing the temperature change required by nitinol. You run power through the nitinol itself, it is heated due to resistance, and then you get the phase change that provides the motion you are after. The response was very rapid (for small pieces of metal). I could see where this might not work for large cross sections, or low ambient temperatures. -- Dan Liddell UUCP decwrl!teda!dll TELEPHONE 4089805200 USA curb your dogma. The opinions and views expressed are Dan's.
Technical Details
Message-ID:
<17039@teda.UUCP>Path:
arc1-ca.pugleaf.net!utzoo!utgpu!news-server.csri.toronto.edu!cs.utexas.edu!usc!apple!netcom!teda!dllReferences:
<1990Nov11.205704.24949@watmath.waterloo.edu> <437@psitech.com>Show Full Headers
Complete Article Headers
Path: arc1-ca.pugleaf.net!utzoo!utgpu!news-server.csri.toronto.edu!cs.utexas.edu!usc!apple!netcom!teda!dll From: dll@teda.UUCP (Dan Liddell) Newsgroups: comp.robotics Subject: Re: Nitinol message Message-ID: <17039@teda.UUCP> Date: 19 Nov 90 17:40:58 GMT References: <1990Nov11.205704.24949@watmath.waterloo.edu> <437@psitech.com> Distribution: comp Organization: Teradyne EDA, Inc. Lines: 11