Re:microwave measurements on polymers

#101
From: Nicholas Hauser
Date: Mon, 10 Aug 1992 01:00
12 lines
885 bytes
Hello Rick,
	I used to work with the Dielectrics group at the Division of 
Applied Physics, National Measurement Laboratory, Lindfield, NSW.
Australia.
They did alot of microwave work on polyethylene, used as cable dielectric
for undersea trunk links (pre optic fibre). I think the name of the guy
was Steve Filipzuc (spelling?). Might be worth sending him a letter.

Nick Hauser.

(tried to email using the address given, but didn't work.)
Technical Details
Message-ID: <1992Aug10.010032.23143@newshost.anu.edu.au>
Path: arc1-ca.pugleaf.net!sparky!uunet!munnari.oz.au!manuel!rsphy1.anu.edu.au!nxh109

Show Full Headers
Complete Article Headers
Newsgroups: sci.materials
Path: arc1-ca.pugleaf.net!sparky!uunet!munnari.oz.au!manuel!rsphy1.anu.edu.au!nxh109
From: nxh109@rsphy1.anu.edu.au (Nicholas Hauser)
Subject: Re:microwave measurements on polymers
Message-ID: <1992Aug10.010032.23143@newshost.anu.edu.au>
Sender: news@newshost.anu.edu.au
Reply-To: nxh109@rsphy1.anu.edu.au (Nicholas Hauser)
Organization: Australian National University
Date: Mon, 10 Aug 92 01:00:32 GMT
Lines: 12