In article <1992Oct2.113921.2739@mtroyal.ab.ca>, dhayward@mtroyal.ab.ca writes:
>For years I have been interested in the present and future uses of
>Berrylium. Due to it's many spectacular properties it should be more
>common than it is. any info?
>
Beryllium oxide is used as the electrical insulator and thermal conductor
between electrified electronic devices generating heat and their heat sinks.
If you look in the right trade mags, for example Microwaves&RF (maybe
Photonics Spectra) you can find mention of these things.
(from my husband, Eric Christenson, an Engineer)
--
~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~
Penelope E. Smith PS02@NS.CC.LEHIGH.EDU
Department of Mathematics PS02@LEHIGH.BITNET
Lehigh University
Bethlehem, PA
Technical Details
Message-ID:
<1992Oct7.222241.148720@ns1.cc.lehigh.edu>Path:
arc1-ca.pugleaf.net!sparky!uunet!zaphod.mps.ohio-state.edu!darwin.sura.net!jvnc.net!netnews.upenn.edu!netnews.cc.lehigh.edu!ns1.cc.lehigh.edu!ps02Show Full Headers
Complete Article Headers
Path: arc1-ca.pugleaf.net!sparky!uunet!zaphod.mps.ohio-state.edu!darwin.sura.net!jvnc.net!netnews.upenn.edu!netnews.cc.lehigh.edu!ns1.cc.lehigh.edu!ps02 From: ps02@ns1.cc.lehigh.edu (PENELOPE E. SMITH) Newsgroups: sci.materials Subject: Re: Uses of Be Message-ID: <1992Oct7.222241.148720@ns1.cc.lehigh.edu> Date: 7 Oct 92 22:22:41 GMT Organization: Lehigh University Lines: 19