Can anyone suggest a suitable glue for the construction of Al honeycomb panels with Al skins. The operating environment is the same as that of a car. A glue that doesn't need temperatures above 200 C would be best. Thanks in advance, Stu.
Technical Details
Message-ID:
<10616330.16.718510858@eng2.eng.monash.edu.au>Path:
arc1-ca.pugleaf.net!sparky!uunet!munnari.oz.au!bruce.cs.monash.edu.au!monu6!ctl-g11-19.cc.monash.edu.au!10616330Show Full Headers
Complete Article Headers
Newsgroups: sci.materials Path: arc1-ca.pugleaf.net!sparky!uunet!munnari.oz.au!bruce.cs.monash.edu.au!monu6!ctl-g11-19.cc.monash.edu.au!10616330 From: 10616330@eng2.eng.monash.edu.au (STUART ROBERTS) Subject: Al honeycomb sandwitch panels Message-ID: <10616330.16.718510858@eng2.eng.monash.edu.au> Lines: 6 Sender: news@monu6.cc.monash.edu.au (Usenet system) Organization: Faculty of Engineering, Monash University Date: Thu, 8 Oct 1992 02:20:58 GMT