In article <1992Nov10.210417.21065@bnr.ca>, miking@bnr.ca writes...
{Could anyone supply me with physical constants of silicon nitride? The usual
{standard references (Wolfe, INSPEC, CRC) don't seem to have much related to
{this material. Thanks in advance. Mike King
Silicon nitride Density Elasitc Modulus Poisson's ratio
3.44 304 GPa 0.24
Koop Hardness Modulus of Rupture
2200 414-580 MPa
Electrical Resistivity Thermal Conductivity
>10^12 Ohm-meter 16-33 W/m-K
Coefficient of Thermal Expansion Melting Temperature
3.6 (C)^-1 x10^6 ~1900 C
-Eric
****************************************************************************
Eric W. Stroup Department of Bioengineering
ewstroup@cc.utah.edu 2480 MEB, University of Utah
c-sew@math.utah.edu Salt Lake City, UT 84112
****************************************************************************
Technical Details
Message-ID:
<11NOV199209512202@cc.utah.edu>Path:
arc1-ca.pugleaf.net!sparky!uunet!wupost!zaphod.mps.ohio-state.edu!saimiri.primate.wisc.edu!ames!agate!dog.ee.lbl.gov!hellgate.utah.edu!fcom.cc.utah.edu!cc.utah.edu!ewstroupReferences:
<1992Nov10.210417.21065@bnr.ca>Show Full Headers
Complete Article Headers
Newsgroups: sci.materials Path: arc1-ca.pugleaf.net!sparky!uunet!wupost!zaphod.mps.ohio-state.edu!saimiri.primate.wisc.edu!ames!agate!dog.ee.lbl.gov!hellgate.utah.edu!fcom.cc.utah.edu!cc.utah.edu!ewstroup From: ewstroup@cc.utah.edu (ERIC W. STROUP) Subject: Re: Wanted, physical constants of Si3N4 Message-ID: <11NOV199209512202@cc.utah.edu> News-Software: VAX/VMS VNEWS 1.4-b1 Sender: news@fcom.cc.utah.edu Organization: University of Utah Computer Center References: <1992Nov10.210417.21065@bnr.ca> Date: 11 Nov 1992 09:51 MST Lines: 24