Properties of titanium nitride

#263
From: james blanchard
Date: Wed, 11 Nov 1992 15:56
13 lines
921 bytes
Since there was some response to a recent request for the properties
of silicon nitride, I thought I'd post a similar request.  Does anyone
have any information on the properties of titanium nitride?  I'm
particularly interested in the strength of the material (yield
strength, rupture strength, etc.).  Any numbers and or references
would be helpful.

   Thanks,
--

   jake blanchard -- university of wisconsin - madison
   blanchard@engr.wisc.edu  OR   jake@nucst6.neep.wisc.edu
Technical Details
Message-ID: <JAKE.92Nov11155601@nucst6.neep.wisc.edu>
Path: arc1-ca.pugleaf.net!sparky!uunet!charon.amdahl.com!pacbell.com!ames!elroy.jpl.nasa.gov!usc!sol.ctr.columbia.edu!The-Star.honeywell.com!umn.edu!doug.cae.wisc.edu!jake

Show Full Headers
Complete Article Headers
Newsgroups: sci.materials
Path: arc1-ca.pugleaf.net!sparky!uunet!charon.amdahl.com!pacbell.com!ames!elroy.jpl.nasa.gov!usc!sol.ctr.columbia.edu!The-Star.honeywell.com!umn.edu!doug.cae.wisc.edu!jake
From: jake@nucst6.neep.wisc.edu (james blanchard)
Subject: Properties of titanium nitride
Organization: /usr1/jake/.organization
Distribution: sci
Date: 11 Nov 92 15:56:01
Message-ID: <JAKE.92Nov11155601@nucst6.neep.wisc.edu>
Lines: 14