Re: References on ferrofluids

#307
From: Mahesh S. Khot
Date: Mon, 14 Dec 1992 01:32
41 lines
1773 bytes
In a previous article, me@hamilton.eecs.umich.edu (My Account) says:

>>What you are refering to here is more likely ferrofluids.
>>Electrorheological fluids use electric fields instead of magnetic fields
>>
>>M. Block and J.P. Kelly, "Electro-rheology review article", J. Phys. D:
>>Appl Phys. vol 21, Dec 14, 1988, p. 1661-1677.
>>
>
>Hi everyone,
>
>I looked in several  Physics Journals in order to obtain some 
>articles about this ferrofluids,
>or  materials that harden/soften with applied magnetic field.
>Unfortunately I did nut sucesseed.
>
>I would greatly appreciate any references or pointer.
>
>M. BOUZIT   
>mbouzit@robo.jussieu.fr
>Robotics Lab of Paris
>Universite Piere et Marie Currie
>FRANCE
>
>
>

If Electrorheological Fluids is what you're looking for or something
similar to that there is an article in recent issue of Science, with 34
references.  That should give you a start.
Citation:
Title:		Electrorheological Fluids
Author:		Thomas C. Halsey
Source:		Science Vol 258, 30th October 1992, 761-766. 

Mahesh
-- 
The King of Queen (rock group) is dead / But their music still lingers.
euphemism:  famous dummies =  Madam Tussade's Wax Museum. 
Still at Case msk9@po.cwru.edu
Technical Details
Message-ID: <1ggo6jINNib3@usenet.INS.CWRU.Edu>
Path: arc1-ca.pugleaf.net!sparky!uunet!usc!wupost!zaphod.mps.ohio-state.edu!magnus.acs.ohio-state.edu!usenet.ins.cwru.edu!po.CWRU.Edu!msk9
References: <1992Dec12.163254.2061@zip.eecs.umich.edu>

Show Full Headers
Complete Article Headers
Path: arc1-ca.pugleaf.net!sparky!uunet!usc!wupost!zaphod.mps.ohio-state.edu!magnus.acs.ohio-state.edu!usenet.ins.cwru.edu!po.CWRU.Edu!msk9
From: msk9@po.CWRU.Edu (Mahesh S. Khot)
Newsgroups: sci.materials
Subject: Re: References on  ferrofluids
Date: 14 Dec 1992 01:32:03 GMT
Organization: Case Western Reserve University, Cleveland, OH (USA)
Lines: 41
Message-ID: <1ggo6jINNib3@usenet.INS.CWRU.Edu>
References: <1992Dec12.163254.2061@zip.eecs.umich.edu>
Reply-To: msk9@po.CWRU.Edu (Mahesh S. Khot)
NNTP-Posting-Host: slc5.ins.cwru.edu