I have been experimenting with determining the integrity of cross linked
polymers. So far I have exposing my samples in an oxygen rich plasma etch
for 10 minutes then analyzing the sample in a SEM. I think we are seeing
that examples of proper or "good" cross linked polymers show a grain of
structure of uniform size and orientation while the "bad" samples seem
to display a wide variation of grain size over a given area. Is this a
viable method of analyzing such materials? Can anyone add anything to
this? I am not very familiar with such materials so consider me mostly
ignorant on this subject. Any information (in simple terms) would be of
great help.
Thanks,
******************************************************************
* Dwight Brantley * Failure Analysis & Reliability Dept. *
* Intergraph, Corp. * Reply To: brantley@falab1.b21.ingr.com *
* Huntsville, AL * Voice: 205-730-4456 *
******************************************************************
Technical Details
Message-ID:
<1992Dec15.224100.25463@infonode.ingr.com>Path:
arc1-ca.pugleaf.net!sparky!uunet!infonode!brantleyShow Full Headers
Complete Article Headers
Newsgroups: sci.materials Path: arc1-ca.pugleaf.net!sparky!uunet!infonode!brantley From: brantley@infonode.ingr.com (Dwight D. Brantley) Subject: identifying polymer cross linking Message-ID: <1992Dec15.224100.25463@infonode.ingr.com> Organization: Intergraph Corporation, Huntsville, AL. Distribution: usa Date: Tue, 15 Dec 1992 22:41:00 GMT Lines: 19