Re: Amorphous diamond film

#407
From: Del Cotter
Date: Wed, 27 Jan 1993 13:12
25 lines
1581 bytes
Darin S. Olson writes:
>First off there can not be such a thing as amorphous diamond.  You probably
>realize this, but just in case: Diamond is a crystal therefor can not be 
>amorphous.  Amorphous diamond comes about due to amorphous silicon, which
>does exist.  The correct term would be amorphous sp3 carbon, to distinguish
>it from amorphous sp2 carbon (ie: soot).  

Thank you.  This is exactly the context in which the question came up.
Our lecturer listed:

Graphite			sp2
Amorphous carbon (soot)		sp2 (some sp3)
Diamond				sp3

and we said 'What about sp3 (some sp2)?'
and he said 'Ah! That's amorphous diamond'

Which as you say, sounds like a contradiction in terms.

Thanks also to antoni s gozdz and all who have mailed me; this undergrad's
curiosity is satisfied (for now!).
-- 
 ',' ' ',','  |                                                  |  ',' ' ',','
   ', ,','    |       Del Cotter       mt90dac@brunel.ac.uk      |    ', ,','  
     ','      |                                                  |      ','    
Technical Details
Message-ID: <C1IKo9.Ftv@brunel.ac.uk>
Path: arc1-ca.pugleaf.net!sparky!uunet!news.univie.ac.at!scsing.switch.ch!univ-lyon1.fr!ghost.dsi.unimi.it!rpi!usc!elroy.jpl.nasa.gov!ames!agate!doc.ic.ac.uk!uknet!brunel!mt90dac
References: <1993Jan25.223429.26696@enterprise.rdd.lmsc.lockheed.com>

Show Full Headers
Complete Article Headers
Path: arc1-ca.pugleaf.net!sparky!uunet!news.univie.ac.at!scsing.switch.ch!univ-lyon1.fr!ghost.dsi.unimi.it!rpi!usc!elroy.jpl.nasa.gov!ames!agate!doc.ic.ac.uk!uknet!brunel!mt90dac
From: mt90dac@brunel.ac.uk (Del Cotter)
Newsgroups: sci.materials
Subject: Re: Amorphous diamond film
Keywords: crystalline amorphous carbon diamond sp2 sp3