I have just discovered that 3-n-butyl-pyridine forms a glass
somewhere between 125 K and 150 K. I have been unable to find any
reference giving a value for Tg or even admitting that it forms a glass
(I guessed that it would because butyl benzene does) after searching
through twenty years of Chem Abstracts plus a few other sources. Does
anyone out there have a reference giving Tg for this stuff? Barring
that, does anyone know where I could send a sample to have DSC done
on it? Thanks.
__________________________________________________________________________
John Fourkas jaco@ccwf.cc.utexas.edu
Department of Chemistry spike@d31mf0.stanford.edu
University of Texas at Austin jaco@leland.stanford.edu
Technical Details
Message-ID:
<76767@ut-emx.uucp>Path:
arc1-ca.pugleaf.net!sparky!uunet!wupost!usc!cs.utexas.edu!ut-emx!ccwf.cc.utexas.edu!jacoShow Full Headers
Complete Article Headers
Path: arc1-ca.pugleaf.net!sparky!uunet!wupost!usc!cs.utexas.edu!ut-emx!ccwf.cc.utexas.edu!jaco From: jaco@ccwf.cc.utexas.edu (John T. Fourkas) Newsgroups: sci.materials Subject: Glass transition of 3-n-butyl-pyridine Message-ID: <76767@ut-emx.uucp> Date: 29 Jul 92 20:56:16 GMT Sender: news@ut-emx.uucp Reply-To: jaco@ccwf.cc.utexas.edu (John T. Fourkas) Organization: Dept. of Chemistry, University of Texas at Austin Lines: 14 Originator: jaco@doc.cc.utexas.edu