Re: Insulator with good heat conductivity

#64
From: John Whitmore
Date: Thu, 30 Jul 1992 00:37
19 lines
1364 bytes
In article <17760004@hpnmdla.sr.hp.com> stanb@hpnmdla.sr.hp.com (Stan Bischof) writes:
>In sci.materials, whit@milton.u.washington.edu (John Whitmore) writes:

>>best bet is BeO (highly toxic, by the way!)

>Nonsense. This is pure urban legend. You could eat BeO on your breakfast
>cereal and have no problems.

>The only problems with BeO come in when you powder it very finely and 
>inhale it into your lungs. The small particles cause some nasty reactions
>similar to what happens with inhaled asbestos. Basically a mechanical
>irritation. 

	Are you certain of that?  My trusty TLV-TWA table shows acceptable 
dust levels of arsenic at 0.5 mg/m^3, and of beryllium at 0.002 mg/m^3;
beryllium is a very toxic light-metal poison, and I always thought
the oxide was just as toxic.

	John Whitmore
Technical Details
Message-ID: <1992Jul30.003724.12642@u.washington.edu>
Path: arc1-ca.pugleaf.net!sparky!uunet!cs.utexas.edu!sdd.hp.com!uakari.primate.wisc.edu!usenet.coe.montana.edu!news.u.washington.edu!milton.u.washington.edu!whit
References: <7926@dirac.physics.purdue.edu> <17760004@hpnmdla.sr.hp.com>

Show Full Headers
Complete Article Headers
Path: arc1-ca.pugleaf.net!sparky!uunet!cs.utexas.edu!sdd.hp.com!uakari.primate.wisc.edu!usenet.coe.montana.edu!news.u.washington.edu!milton.u.washington.edu!whit
From: whit@milton.u.washington.edu (John Whitmore)
Newsgroups: sci.materials
Subject: Re: Insulator with good heat conductivity
Message-ID: <1992Jul30.003724.12642@u.washington.edu>
Date: 30 Jul 92 00:37:24 GMT
References: <7926@dirac.physics.purdue.edu> <17760004@hpnmdla.sr.hp.com>
Sender: news@u.washington.edu (USENET News System)
Organization: University of Washington, Seattle
Lines: 19