Hello Rick, I used to work with the Dielectrics group at the Division of Applied Physics, National Measurement Laboratory, Lindfield, NSW. Australia. They did alot of microwave work on polyethylene, used as cable dielectric for undersea trunk links (pre optic fibre). I think the name of the guy was Steve Filipzuc (spelling?). Might be worth sending him a letter. Nick Hauser. (tried to email using the address given, but didn't work.)