Thread View: sci.materials
2 messages
2 total messages
Started by AH Al_ashaab
Mon, 07 Sep 1992 20:29
Design guide from plastic material supliers
Author: AH Al_ashaab
Date: Mon, 07 Sep 1992 20:29
Date: Mon, 07 Sep 1992 20:29
17 lines
1124 bytes
1124 bytes
Hi this the first time for me to use this group and I hope I am not misusing it! I always read in the books or papers that the plastic material suppliers give information about a good design guide of the plastic products such as the best Max. or Min. wall thickness to be used or the length of the wall or the best dimension of a Rib and Boss or the shape of round corner and so on. The reason I am send this message is ask if any body can tell about any plastic material suppliers whom really can give such information. Thanks Ahmed AL-ASHAAB Manuf. Eng Dept., Loughborough Univ of Tech Loughborough, Leics. LE11 3TU, England. EMail: A.H.Al_ashaab@lut.ac.uk OR ahmed@mansun.lut.ac.uk Tel 0509-263171 Ext. 4247 Fax. 0509-267725
Re: Design guide from plastic material supliers
Author: Christopher P. Tully,Pathology,6...
Date: Wed, 09 Sep 1992 13:20
Date: Wed, 09 Sep 1992 13:20
41 lines
2409 bytes
2409 bytes
In article 14386@lut.ac.uk, A.H.Al_ashaab@lut.ac.uk (AH Al_ashaab) writes:
>Hi
>this the first time for me to use this group and I hope I am not
>misusing it!
>I always read in the books or papers that the plastic material
>suppliers give information about a good design guide of the plastic
>products such as the best Max. or Min. wall thickness to be
>used or the length of the wall or the best dimension of a Rib and
>Boss or the shape of round corner and so on. The reason I am
>send this message is ask if any body can tell about any plastic
>material suppliers whom really can give such information.
>
>Thanks
>Ahmed AL-ASHAAB
>Manuf. Eng Dept., Loughborough Univ of Tech
>Loughborough, Leics. LE11 3TU, England.
>EMail: A.H.Al_ashaab@lut.ac.uk OR ahmed@mansun.lut.ac.uk
>Tel 0509-263171 Ext. 4247 Fax. 0509-267725
Actually, If you know what you are asking for, and are persistent
enough, most companies have the info. Other sources:
Plastics Encyclopedia - annualy book with 1/2 to 2 page essays on most
if not all plastics produced in the US. I don't remember off the top
of my head who publishes this, but it has most of what you want. In
addition to the essays, it has massive tables listing properties.
GE plastics database - this is a free online design package produced by
GE. Mail me if you want the subscription info (I don't have it handy
right now).
---
*********************************************************************
Chris(topher) P. Tully <cptully@med.unc.edu>
Univ. of North Carolina - Chapel Hill 1122 Vic Charles Dr.
Department of Pathology Raleigh, NC 27606
CB# 7525 work: (919) 966-2699
Chapel Hill, NC 27599 hone: (919) 851-8816
*********************************************************************
I get paid for my opinions, but that doesn't mean that UNC or anybody
else agrees with them.
Thread Navigation
This is a paginated view of messages in the thread with full content displayed inline.
Messages are displayed in chronological order, with the original post highlighted in green.
Use pagination controls to navigate through all messages in large threads.
Back to All Threads