Might anyone know of commercial sources for thin (and preferably single
crystal) FREESTANDING (i.e., unsupported by a substrate)
metal films, say 1000 A to a few microns?  

I have been told someone at the University of Denmark (?) routinely
produces high quality thin metal films, but I don't know the details
or whether anyone else produces these as well.

Many thanks!
Re: SEEKING SOURCE FOR THIN METAL FILMS
#180
Author: Scott D. Berry
Date: Thu, 27 Aug 1992 14:22
27 lines
1853 bytes
In article <Btn89J.MG6@news.cso.uiuc.edu> ritley@uiucmrl.bitnet () writes:
>
>
>Might anyone know of commercial sources for thin (and preferably single
>crystal) FREESTANDING (i.e., unsupported by a substrate)
>metal films, say 1000 A to a few microns?  
>
Free standing foils (polycrystalline) are routine in the nuclear and
high energy atomic collision physics community -- you buy films deposited
on glass slides, float them off onto the surface of water, and then pick them
up (VERY carefully, especially if only 200 A) onto a holder.  Talk to 
your nearest accelerator jockeys for the latest info about sources.

As far as single crystal films, they do exist -- I have been on experiments
using them (years ago), but I have no idea where the best sources are.
I would expect if you found out typical sources of the polycrystalline films
the suppliers would know who does the single crystal foils.

>I have been told someone at the University of Denmark (?) routinely
>produces high quality thin metal films, but I don't know the details
>or whether anyone else produces these as well.
>
>Many thanks!

Scott D. Berry    Assistant Professor of Physics    Florida State University
315 Keen Bldg, B-159, Tallahassee, FL 32306-3016    (904) 644-1218
INTERNET:   berry@redbeard.physics.fsu.edu    BITNET:   berry@fsu
Thread Navigation

This is a paginated view of messages in the thread with full content displayed inline.

Messages are displayed in chronological order, with the original post highlighted in green.

Use pagination controls to navigate through all messages in large threads.

Back to All Threads